Aging-Induced Changes in Optical Behavior and Surface Morphology of Additively and Subtractively Manufactured Dental Materials
Georgiana Osiceanu, Roxana Diana Vasiliu, Flavia Roxana Bejan, Mihaela Ionela Gherban, Liliana Porojan
Victor Babeș University of Medicine and Pharmacy Timișoara · National Institute of Research and Development for Electrochemistry and Condensed
Key points
From the paper's conclusion- Therefore, the objectives of this study were to evaluate the optical and surface characteristics of six computer-aided design/Computer-Aided Manufacturing (CAD-CAM) dental materials, both subtractive and additive, in relation to in vitro degradation.
Abstract
Background/Objectives: Modern dentistry focuses on the ongoing development of digital alternative technologies and the study of the properties of these innovative materials is deemed essential. Therefore, the objectives of this study were to evaluate the optical and surface characteristics of six computer-aided design/Computer-Aided Manufacturing (CAD-CAM) dental materials, both subtractive and additive, in relation to in vitro degradation. Methods: CAD-CAM dental materials, subtractively processed (Vita Enamic, Cerasmart, Brilliant and Tetric) and additively manufactured (Saremco Crowntec and Voco C&B), were prepared to standard dimensions of 14 × 10 × 1 mm, with baseline measurements taken prior to, and after, the degradation procedures, consisting of immersion in an ADA-recommended staining broth, artificial aging (thermocycling), and the combined effects of staining and in vitro aging. Additionally, two different surface treatments were investigated (polished and glazed). Results: The poorest color stability was observed for Tetric glazed specimens (mean value 25.585) subjected to staining, while the best performance was recorded for Brilliant polished Control (average value of 0.781). The staining procedure produced the most pronounced color changes. Surface treatment did not significantly affect color stability, and surface roughness was not influenced by either the degradation method or the surface treatment (p > 0.05). Atomic Force Microscopy (AFM) evaluation revealed superior performance of the glazed surfaces, characterized by lower nanoroughness values compared with polished surfaces and a smoother surface appearance. Conclusions: The staining potential of staining broth was demonstrated in this study, with the highest values recorded after the staining procedures. In addition, the influence of artificial aging alone and artificial aging combined with staining was investigated, providing relevant results for a better clinical approach. Moreover, surface treatment demonstrated reliability and therefore clinical applicability.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Color stability of CAD/CAM and additively manufactured resin materials: influence of surface treatment and layer thickness - an in vitro studyThe Saudi Dental Journal · 2026
- Artificial Aging and Its Impact on Surface Properties of Conventional and CAD-CAM Occlusal Splint Materials: An In Vitro Comparative Study.International journal of dentistry · 2026
- Color Stability and Surface Roughness of CAD/CAM Hybrid Ceramics and Resin Composites After Simulated Toothbrushing in Coffee: An In Vitro StudyApplied Sciences · 2026
- Cross-Sectional Characterization of Stain Retention and Glaze Alteration in 3D-Printed and Milled Hybrid Dental MaterialsJournal of Functional Biomaterials · 2026
- Effect of surface treatment protocols and thermocycling on the optical, surface, and mechanical properties of additively manufactured resin materials.Clinical oral investigations · 2026
- Are there differences in the optical properties of subtractively and additively manufactured zirconia restorations? A systematic review and meta-analysis.The Journal of prosthetic dentistry · 2026