Effect of surface treatment protocols and thermocycling on the optical, surface, and mechanical properties of additively manufactured resin materials.
Esra Cengiz-Yanardag, Ayse Tugba Erturk-Avunduk, Ezgi Guven
Department of Restorative Dentistry, Faculty of Dentistry, Mersin University, Mersin, Türkiye. esracengiz@mersin.edu.tr. · Department of Restorative Dentistry, Faculty of Dentistry, Mersin University, Mersin, Türkiye.
Key points
From the paper's conclusion- Surface treatments and thermocycling significantly affect additively manufactured resins; mechanical pretreatments improve hardness but may compromise optical properties.
Abstract
OBJECTIVES: This study evaluated the effects of surface treatment protocols and thermocycling on the optical, surface, and mechanical properties of additively manufactured resins. MATERIALS AND METHODS: Five materials (saremco print CROWNTEC, VarseoSmile Crownplus, VarseoSmile TriniQ, VarseoSmile TriniQ for Formlabs, and Ceramic Crown) were assigned to six groups: control, silane, sandblasting (SB), SB+silane, hydrofluoric acid (HFA), and HFA+silane. After surface treatments and 5,000 thermocycles, color change (ΔE₀₀), translucency (ΔTP₀₀), gloss, surface roughness (Ra), and microhardness (VHN) were measured. Data were analyzed using robust ANOVA and aligned rank transform (ART) mixed ANOVA with Holm-adjusted multiple comparisons (α = 0.05). RESULTS: Material type, surface treatment, and aging significantly affected all evaluated parameters (p < 0.001). Following surface treatment (T1), SB and SB + S groups exhibited significantly higher surface roughness and microhardness compared with control, silane, HFA, and HFA + S groups (p < 0.001). In terms of ΔE₀₀, SB and SB + S groups exceeded the clinical acceptability threshold (ΔE₀₀ > 1.8), whereas C, S, HFA, and HFA + S groups remained below the perceptibility threshold at T1. After thermocycling (T2), clinically unacceptable color changes were observed in most treatment groups, gloss values decreased significantly, and microhardness increased (p < 0.001). ΔTP₀₀ values were significantly influenced by material type (p < 0.001) but not consistently by surface treatment. Gloss values decreased significantly over time (p < 0.001), with the lowest values observed at T2. Among the materials, Ceramic Crown showed significantly higher microhardness and lower color change compared with the others (p < 0.05). CONCLUSIONS: Surface treatments and thermocycling significantly affect additively manufactured resins; mechanical pretreatments improve hardness but may compromise optical properties. CLINICAL RELEVANCE: Careful selection of surface treatment protocols is required to achieve a balance between mechanical performance and esthetic outcomes in additively manufactured restorations.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Effect of modified glaze application protocols on color stability of 3D-printed permanent dental resinsBMC Oral Health · 2026
- Effect of thermocycling and polishing protocols on the optical and mechanical properties of different CAD-CAM and 3D-printed materials.American journal of dentistry · 2026
- Effect of surface finishing procedures on the color stability of a 3D-printed permanent resin material in artificial saliva at different pH levels: an in vitro study.BMC oral health · 2026
- Gloss and Surface Roughness of Stained and Polished 3D-Printed Resins Used for the Fabrication of Hybrid Denture Prosthesis: An In Vitro Study.Journal of functional biomaterials · 2026
- Erosive-Abrasive Effects on Surface, Mechanical, and Optical Properties of 3D-Printed Resin Composites for Prosthetic Applications.The International journal of prosthodontics · 2026
- Effect of air-borne particle abrasion and tribochemical silica coating on surface characteristics, mechanical behavior, and bonding performance of 3D-printed resin-based materials.Clinical oral investigations · 2026