Source-Dependent Performance of Calcium Silicate-Based Co-Products Derived from Phosphoric Acid Production Processes
Samantha R. Doughty, Shubham Mishra, Clarke J. Summers, Brett Q. Tempest, Jamshid Armaghani, Mark Vignovic, Tara L. Cavalline
Key points
From the paper's conclusion- These results indicate that phosphogypsum-derived J-Rox use in concrete materials shows promise, particularly when used in ternary, performance-engineered blended binder systems.
Abstract
The phosphate fertilizer industry generates large quantities of phosphogypsum, motivating beneficial-use pathways that convert phosphate-industry residuals into construction materials. This study evaluated calcium silicate-rich J-Rox co-products produced through two source routes: phosphate ore-derived J-Rox from the phosphoric acid production route (JR-P) and phosphogypsum-derived J-Rox from the phosphogypsum recovery route (JR-G). Finely ground J-Rox was examined as a supplementary cementitious material through a staged paste–mortar–concrete framework, while coarsely ground phosphogypsum-derived J-Rox sand was evaluated as a prewetted internal curing aggregate. Paste testing assessed setting behavior, mortar testing evaluated workability-controlled compressive strength and sulfate attack resistance, and concrete testing validated JR-G materials (JR-G1 and JR-G2) in binary, ternary J-Rox–slag, and internally cured systems. JR-P materials produced more systematic setting delay, likely influenced by higher P2O5 contents, while JR-G materials showed more variable but practical setting behavior. Mortar strength results were material- and dosage-dependent, with 15% replacement giving the most consistent response. Sulfate expansion provided the clearest source-route distinction: all JR-G mixtures remained below the 0.1% expansion threshold at 26 weeks, with an average expansion of 0.0560%, while five of the six JR-P mixtures exceeded this threshold, with an average expansion of 0.1499%. At the concrete scale, binary JR-G mixtures achieved practical 28-day strength, with the 15JR-G2 mixture reaching 7593 psi at 91 days compared with 6694 psi for the OPC control. Ternary mixtures containing 15% JR-G and 35% slag showed strong later-age strength gain, increased surface resistivity, and reduced drying shrinkage at 50% OPC replacement. Specifically, the 15JR-G2/35S mixture achieved a 91-day compressive strength of 7372 psi, while the 15JR-G1/35S mixture exhibited a 112-day drying shrinkage of −0.011%, compared with −0.066% for the OPC control. These results indicate that phosphogypsum-derived J-Rox use in concrete materials shows promise, particularly when used in ternary, performance-engineered blended binder systems.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Development of Alkali-Activated Phosphogypsum Mortar Incorporating Silica Fume and Metakaolin for Enhanced Durability and CO 2 MineralisationIOP Conference Series: Earth and Environmental Science · 2026
- Research and Advances in the Application of Phosphogypsum in Pavement Base Course and Subgrade: A ReviewApplied Research · 2026
- Получение карбоната кальция с заданными свойствами крупности как фактор эффективной утилизации техногенного гипсосодержащего сырьяJournal of Mining Institute · 2026
- Gel-Dominated Microstructural Evolution and Strength Development in Phosphogypsum-Based PRBA Systems for Road Base Applications.Gels (Basel, Switzerland) · 2026
- Preparation, Hydration Characteristics, and Carbon Footprint Assessment of Sulfoaluminate Cement Prepared by Co-Utilization of Industrial Solid Wastes and BauxiteMaterials · 2026
- Mineral reconstruction of high-volume phosphogypsum driven by a slag-based composite stabilizer: mechanisms of subgrade performance enhancement and phosphorus/fluoride immobilization.Journal of hazardous materials · 2026