Coatings

Membrane, Air, and Water Curing of GGBS and Microsilica Concrete: Age-Dependent Strength Penalty and Carbon Cost

Christelle Tohme, Wadhha Alotaibi, Rayan Aljabaah, Shahad Alghanim, Farah Alazmi, Yasmeen Alrasheedi, Jacqueline Saliba

Key points

From the paper's conclusion
  • We tested whether this holds for ordinary Portland cement (OPC), 50% ground granulated blast furnace slag (GGBS), and 7% microsilica (MS) concretes cured in water or exposed outdoors for 20 days, bare or under a membrane-forming curing compound, and whether water curing repays its carbon cost.

Abstract

In water-scarce regions, curing water is often desalinated, yet curing of blended concrete is judged on 28-day strength. We tested whether this holds for ordinary Portland cement (OPC), 50% ground granulated blast furnace slag (GGBS), and 7% microsilica (MS) concretes cured in water or exposed outdoors for 20 days, bare or under a membrane-forming curing compound, and whether water curing repays its carbon cost. Strength was measured at 7, 28 and 90 days, alongside absorption, sorptivity, microstructure, and a life-cycle assessment including curing. The curing penalty reversed with age: GGBS concrete was most affected at 7 days (retention 0.63–0.64) but recovered to 0.89–0.96, whereas MS concrete retained 0.94–0.95 at 28 days and fell to 0.83–0.85 at 90 days. A Eurocode 2-type function fitted at 7 and 28 days predicted 90-day water-cured strength within 7% but erred by up to 18% for non-water-cured blended concrete. Desalinated curing water added at most 2.4% to global warming potential per cubic meter, whereas non-water curing raised it per MPa by up to 28%; except for OPC at 7 days, water curing stayed lower-carbon unless its burden was 1.9–24 times higher. Blended-concrete curing should be specified per binder and verified beyond 28 days.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers