IOP Conference Series: Earth and Environmental Science

Mechanical and Durability Behaviour of Seawater Mixed Recycled Brick Aggregate Concrete

T. U. Mohammed, Z. Fariha, M. A. Rony

Key points

From the paper's conclusion
  • Overall, suitable combinations of slag replacement and cement content allow seawater to be used in concrete without reducing mechanical performance.

Abstract

This study investigates the mechanical and durability performance of concrete utilizing seawater and recycled brick aggregates as alternatives to freshwater and natural coarse aggregates, respectively. The study was conducted using 340, 400, and 450 kg/m 3 binder contents, with GGBFS replacing CEM Type I cement at levels of 30% and 70% by volume. Five mix cases were prepared using 100% recycled brick aggregates, where mix with freshwater served as the control mix. Slump test results ranged from 83 to 148 mm. Compressive strength and ultrasonic pulse velocity were assessed after 7 and 28 days of curing, while split tensile strength was measured after 28 days. At 28 days, seawater concrete containing 30% slag and 340 kg/m 3 cement content exhibited an 11.63% strength gain in compressive strength compared with control mix, while a similar mix with 450 kg/m 3 binder content and 70% slag achieved approximately 97% strength of the control mix. Split tensile strengths ranged from 3 to 7 MPa. UPV results indicated good concrete quality, while rapid chloride permeability test results indicated very low chloride ion penetrability with increasing cement content and slag replacement. Overall, suitable combinations of slag replacement and cement content allow seawater to be used in concrete without reducing mechanical performance.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers