Effect of Laser Post-Treatment on the Microstructure, Mechanical and Tribological Properties of Detonation- and Flame-Sprayed Ni–Cr–Fe–Si–B–C Coatings
Dastan Buitkenov, Nurmakhanbet Raisov, Aiym Nabioldina, Dosym Yerbolatuly, Nurkhat Bimakhan
Key points
From the paper's conclusion- These findings demonstrate that laser post-treatment can improve the mechanical and tribological performance of self-fluxing Ni–Cr–Fe–Si–B–C coatings, with the magnitude and nature of these improvements depending on the initial microstructure formed by the respective spraying method.
Abstract
This study investigates the effect of laser post-treatment on the microstructure, phase composition, mechanical, and tribological properties of self-fluxing Ni–Cr–Fe–Si–B–C coatings deposited by detonation spraying (DS) and gas-flame spraying (GFS) onto AISI 321 stainless steel substrates. The coatings before and after laser treatment (LT) were examined using scanning electron microscopy, energy-dispersive X-ray spectroscopy, X-ray diffraction, instrumented indentation, and ball-on-disk tribological testing. The as-deposited coatings were characterized by a dense structure and low porosity, amounting to 0.306 ± 0.014% for the DS coatings and 0.433 ± 0.011% for the GFS coatings. Phase analysis revealed a multiphase structure consisting predominantly of a γ-(Ni,Fe) matrix reinforced by Cr7C3 carbide, CrB and Ni3B borides, as well as Ni31Si12 silicide. After laser treatment, the main crystalline phases were preserved; however, changes in the relative intensities of the diffraction peaks were observed, suggesting microstructural modifications during rapid melting and subsequent solidification. The mechanical response to laser treatment depended on the coating deposition method. For the DS coating, Vickers hardness increased from 1049.1 ± 43.4 to 1206.1 ± 63.1 HV, while the elastic modulus increased from 233.6 ± 6.2 to 258.4 ± 5.3 GPa. For the GFS coating, hardness increased from 1096.2 ± 58.8 to 1121.3 ± 49.1 HV, whereas the elastic modulus decreased from 228.0 ± 5.9 to 187.0 ± 8.8 GPa. Laser treatment also improved the wear resistance of both coating types. The wear rate of the DS coating decreased from 1.939 × 10−4 to 1.465 × 10−4 mm3/(N × m), while that of the GFS coating decreased from 2.419 × 10−4 to 1.476 × 10−4 mm3/(N × m), corresponding to reductions of approximately 24% and 39%, respectively. Under dry sliding conditions, the coefficient of friction of the DS coating remained nearly unchanged after laser treatment, decreasing slightly from 0.627 to 0.620, whereas that of the GFS coating decreased from 0.623 to 0.582. These findings demonstrate that laser post-treatment can improve the mechanical and tribological performance of self-fluxing Ni–Cr–Fe–Si–B–C coatings, with the magnitude and nature of these improvements depending on the initial microstructure formed by the respective spraying method.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Effect of Laser Remelting on the Microstructure, Mechanical and Tribological Properties of Detonation-Sprayed NiCrFeBSiC Coatings for Mechanical Engineering ApplicationsJournal of Manufacturing and Materials Processing · 2026
- Effect of Vacuum Heat Treatment on the Structural-Phase State of Detonation-Sprayed NiCrAl Coatings.Materials (Basel, Switzerland) · 2026
- Tribological Properties of Flame-Sprayed Fe-Based Composite Coatings Synergistically Enhanced by NiCr-Cr3C2 and Ni-MoS2.Materials (Basel, Switzerland) · 2026
- A critical analysis of the scratch test for thermally sprayed coatingsThe International Journal of Advanced Manufacturing Technology · 2026
- Factorial Experiments on Laser Pre‐Treatment of Low‐Carbon Steel Welds Prior to the Application of Organic CoatingsMaterials and Corrosion · 2026
- Effect of Laser Cladding with Constant Specific Energy on the Hardness and Friction Properties of Stellite 21 Coatings on AISI 304 Stainless SteelCoatings · 2026