Microstructural Evolution and Failure Mechanisms of Plasma-Sprayed Pure Si and Si–15 mol% HfO2 Bond Coatings in Dry-Oxygen and Water-Vapor Environments at 1623 K
Jianhai Yu, Juhan Yang, Zhongshen Dong, Kunying Ding, Taotao Cheng, Fulin Zhu, Tao Zhang, Yi Jiang,
Key points
From the paper's conclusion- These findings inform the compositional optimization and structural design of Si-based bond coats for ultra-high-temperature water-vapor service.
Abstract
To address the softening and limited oxidation and water-vapor corrosion resistance of Si bond coats at ultra-high temperatures, Si and Si–15 mol% HfO2 (denoted 15HS) composite bond coats were deposited on pressureless sintered SiC substrates by air plasma spraying (APS). Their phase evolution, cross-sectional microstructure, and failure mechanisms were examined after 20–200 h at 1623 K in dry oxygen and in a 90% H2O–10% O2 environment. In dry oxygen, a SiO2 thermally grown oxide (TGO) layer formed on the Si coating surface, cracked and spalled with time, and the coating thinned progressively. In the 15HS coating, HfO2 reacted in situ with SiO2 to form HfSiO4; the combined volume expansion and spallation resistance of the dense layer caused the coating to thicken rather than thinning, and the TGO remained dense and crack-free. Under water-vapor corrosion, the Si coating was continuously consumed through gas-phase volatilization of SiO2 as Si(OH)4, accompanied by porosity and through-thickness cracks; after 200 h the coating thickness was only ~70% of the initial value. The 15HS coating instead underwent a three-stage evolution—homogeneous oxidation, layered construction, and barrier stabilization—after which a dense double-layer barrier formed, with an outer HfSiO4 layer and an inner SiO2 band, giving a thickness retention of ~90%, well above that of the Si coating. Mechanistic analysis showed that HfO2 particles remained in place while Si4+ diffused outward and converted to HfSiO4 at the HfO2 surface. HfSiO4 protected the coating through two mechanisms: blocking OH−/H2O diffusion pathways and suppressing Si(OH)4 volatilization. These findings inform the compositional optimization and structural design of Si-based bond coats for ultra-high-temperature water-vapor service.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Development of Oxide Dispersion Strengthened Bondcoats by High-Velocity Air Fuel SprayingJournal of Thermal Spray Technology · 2026
- Self‐Healing and Corrosion Resistance of TiSi 2 ‐Modified Yb 2 Si 2 O 7 Environmental Barrier CoatingsJournal of the American Ceramic Society · 2026
- Effect of He Addition on the In‐Flight Behavior of ZrSiO 4 Powder and Coating Deposition During DC Arc Plasma SprayingJournal of the American Ceramic Society · 2026
- The oxidation resistance of Hf‐Ta‐Si‐B‐O glass film reinforced ZrB₂ –SiC coating in wide temperature range environmentsJournal of the American Ceramic Society · 2026
- Stability behavior of a novel 3DC C/Y2Si2O7 composites in vacuum at high temperatureJournal of Materials Research and Technology · 2025
- Reaction Kinetics of Yb 2 Si 2 O 7 –Yb 2 SiO 5 Mixtures in High‐Temperature Water Vapor EnvironmentsJournal of the American Ceramic Society · 2026