Journal of the American Ceramic Society

Reaction Kinetics of Yb 2 Si 2 O 7 –Yb 2 SiO 5 Mixtures in High‐Temperature Water Vapor Environments

C. S. Witharamage, W. Jackson, E. J. Opila

Key points

From the paper's conclusion
  • Among all the compositions, YbDS + 10% fine YbMS shows the most resistance to water vapor attack due to the uniform distribution of YbMS in the YbDS matrix and low porosity microstructure.

Abstract

Thermochemical stability of Yb 2 Si 2 O 7 (YbDS) + x % ( x = 10 and 30 vol.%) Yb 2 SiO 5 (YbMS) mixtures was investigated in high‐velocity water vapor (∼200 m s −1 ) at 1300°C and 1400°C. YbDS + x % YbMS coupons were synthesized by dispersing 10 and 30 vol.% YbMS in a YbDS matrix. Scanning electron microscopy and x‐ray diffraction analysis revealed silica depletion from the YbDS matrix, forming YbMS in all YbDS + x % YbMS materials after exposure to high‐velocity steam at 1300°C and 1400°C. The thickness of the reaction‐product layer of each material system was measured as a function of exposure time and temperature. The reaction kinetics were parabolic for all YbDS + x % YbMS samples at 1300°C and 1400°C. Among all the compositions, YbDS + 10% fine YbMS shows the most resistance to water vapor attack due to the uniform distribution of YbMS in the YbDS matrix and low porosity microstructure.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.