Two-Step Sintering and Sr(Fe0.5Nb0.5)O3 Addition Enhancing Electrical Properties of KNN-Based Lead-Free Piezoelectric Ceramics
Yafei Miao, Shaohua Su, Bijun Fang, Shuai Zhang, Xiaolong Lu, Jianning Ding
Key points
From the paper's conclusion- These changes directly tailor the electrical properties: the near-room-temperature O-T boundary at x = 0.03 gives the best soft-type response (piezoelectric constant d33 = 133 pC/N, electromechanical coupling coefficient Kp = 0.285, remnant polarization Pr = 22.72 μC/cm2), whereas acceptor-oxygen-vacancy dipoles at x = 0.01 pin domain walls, yielding the highest mechanical quality factor Qm = 329
Abstract
Lead-free (1−x)(K0.49Na0.51)(Nb0.95Sb0.05)O3−xSr(Fe0.5Nb0.5)O3 [(1−x)KNNbS−xSrFNb, x = 0.01–0.07] ceramics with 0.5 wt% CuO were prepared by conventional sintering (CS) and two-step sintering (TSS). Increasing the SrFNb content drives the structure from orthorhombic–tetragonal (O-T, x ≤ 0.03) coexistence to rhombohedral–tetragonal (R-T, x ≥ 0.05) coexistence, and shifts the phase boundary toward room temperature, while Fe3+/Nb5+ B-site disorder induces polar nanoregions, diffuse dielectric behavior (dispersion index γ > 1.7) and a drop of Tm (temperature of dielectric constant maximum) from 295 °C to below room temperature. Increasing SrFNb significantly reduces the average grain size from 0.6 μm to 0.3 μm, while TSS decouples densification from grain growth, raising the maximum relative density from 92.13% to 94.51% at x = 0.05 with only a slight reduction in average grain size from 0.35 μm to 0.32 μm. These changes directly tailor the electrical properties: the near-room-temperature O-T boundary at x = 0.03 gives the best soft-type response (piezoelectric constant d33 = 133 pC/N, electromechanical coupling coefficient Kp = 0.285, remnant polarization Pr = 22.72 μC/cm2), whereas acceptor-oxygen-vacancy dipoles at x = 0.01 pin domain walls, yielding the highest mechanical quality factor Qm = 329 with low tanδ, and TSS further improves fatigue resistance. Combining SrFNb-driven structural evolution with TSS microstructural control thus offers an effective route to tailor KNN-based lead-free piezoelectrics.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Enhanced Extrinsic Piezoelectric Contribution and Microscopic Origin of Grain Size Effect in Lead-Free KNN-Based Ceramics.ACS applied materials & interfaces · 2026
- Effects of Sintering Processes and Poling Conditions on the Piezoelectric Coefficient d 33 of Na 0.5 K 0.5 NbO 3 -BiFeO 3 CeramicsJournal of Physics: Conference Series · 2026
- Gradient‐Acceptor‐Doping Breaks the Piezoelectric Trade‐Off in Lead‐Free (K, Na)NbO₃ CeramicsAdvanced Materials · 2025
- Tailoring KNN ceramics through metal oxide doping: a comprehensive review on structure-property relationships and energy harvesting applications.Nanoscale · 2026
- Ultra‐Low Dielectric Loss and High Depolarization Temperature Achieved in (K,Na)NbO₃ ‐Based Piezoceramics via Modulating Carrier Migration and Domain DynamicsAdvanced Energy Materials · 2026
- Synergistic Domain and Defect Engineering Enables Giant Electrostrain With High Piezoelectric Sensitivity in Lead‐Free FerroelectricsSmall · 2026