Effects of Sintering Processes and Poling Conditions on the Piezoelectric Coefficient d 33 of Na 0.5 K 0.5 NbO 3 -BiFeO 3 Ceramics

Hong Chen, Yi Wu, Xinyan Zhang, Yi Wu, Yuanmou Li, Xiaoyang Liu

Key points

From the paper's conclusion
  • The optimum processing conditions for (1− x ) NKN- x BiFeO 3 ceramics are determined as follows: sintering at 1150 °C for 5 h, poling at 30 kV/cm, 120 °C for 25 min, yielding a d 33 of 181 pC/N.

Abstract

Lead-free piezoelectric ceramics (1− x )Na 0.5 K 0.5 NbO 3 - x BiFeO 3 were prepared by a conventional electronic ceramic preparation process. The effects of sintering temperature, holding time, poling electric field, poling temperature, and poling time on the piezoelectric coefficient d 33 of the ceramics were investigated. The results show that the composition with x =0.006 achieved the highest piezoelectric coefficient d 33 (181 pC/N) when sintered at 1150 °C for 5 h. At room temperature, the P - E hysteresis loops indicate that the coercive field E c of the ceramics is approximately 12∼18 kV/cm, and a poling electric field of 1.2∼1.6 times E c is required to achieve sufficient electric domain orientation. The piezoelectric coefficient d 33 reaches its optimum at a poling temperature of 120∼150 °C, beyond which thermal depolarization causes a decline in d 33 ; the optimal poling time is 25∼30 min, and excessive poling duration leads to depolarization due to space charge accumulation. The optimum processing conditions for (1− x ) NKN- x BiFeO 3 ceramics are determined as follows: sintering at 1150 °C for 5 h, poling at 30 kV/cm, 120 °C for 25 min, yielding a d 33 of 181 pC/N.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers