Mechanical Properties and Durability Analysis of Hematite Concrete After High-Temperature Exposure
Youjia Zhang, Yilong Li, Junhao Zhang
Key points
From the paper's conclusion- The results show that the mass loss ratio of hematite concrete increases continuously with the rise in exposure temperature.
Abstract
In this study, hematite was adopted as both coarse and fine aggregates to prepare hematite concrete with three strength grades of C40, C50 and C60. Specimens of hematite concrete subjected to five temperature levels were tested for mass loss ratio, compressive strength and flexural strength. Durability tests including chloride penetration test and sulfate attack test were also carried out. The results show that the mass loss ratio of hematite concrete increases continuously with the rise in exposure temperature. At 600 °C, the residual compressive strength ratios of C40, C50 and C60 specimens are 55.15%, 61.85% and 64.02%, respectively. At 450 °C, the flexural strength of specimens of all three strength grades retains only approximately 50% of the room-temperature value. This indicates that flexural performance is more sensitive to thermal damage than compressive performance. After high-temperature exposure, the chloride diffusion coefficient increases exponentially with temperature. At 600 °C, the diffusion coefficients of C40, C50 and C60 specimens are about 30 times those at room temperature. The pore sizes of specimens under ambient temperature are mainly distributed in the range of 10–100 nm. After high-temperature exposure, the proportion of small pores decreases, while the proportion of harmful pores with pore size larger than 1000 nm increases. At 600 °C, the pore size distribution shifts toward the range of 1000–10,000 nm. Within the temperature range of 25–300 °C, the corrosion resistance coefficients of all specimens remain above 95%, demonstrating excellent sulfate attack resistance in this temperature interval. At 450 °C, the corrosion resistance coefficient decreases continuously with the extension of erosion age. At 600 °C, the corrosion resistance coefficient of C40 specimens drops to 73.2%, below the durability threshold.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Residual physio-mechanical properties and degradation analysis of foamed concrete exposed to elevated temperaturesScientific Reports · 2025
- Post-Heating Performance of Concrete Containing Grading-Controlled Recycled Refractory Brick Fine AggregateConstruction Materials · 2026
- In Situ Study on High-Temperature Performance and Structural Deterioration Mechanism of ConcreteProcesses · 2026
- High-Temperature Performance of Metakaolin-Based Geopolymer Recycled Mortar with Pumice Powder.Materials (Basel, Switzerland) · 2026
- Dynamic mechanical properties and constitutive modeling of red sandstone after high-temperature treatment under different confining pressures: Micromechanical perspectiveResults in Engineering · 2026
- Multiscale Evaluation of the High-Temperature Performance of Cement Mortars Containing Class C and F Fly Ash.Materials (Basel, Switzerland) · 2026