Investigation of the Causes of Web Cracking and Strengthening Methods for Continuous Box-Girder Bridges with Large Cantilevers and Thin Web
Jianzhen Wu, Juanjuan Chen, Jinlong Huang, Xiangyu Han, Yang Jiang, Qu Wang
Key points
From the paper's conclusion- The results indicate that long-term prestress loss reduces the compressive stress reserve in the box-girder section and is a primary contributor to transverse cracking at the girder bottom, whereas inclined web cracking is primarily caused by the combined effects of shear stress and vertical tensile stress.
Abstract
To address structural deficiencies—including web cracking, transverse cracking at the girder bottom, and inadequate load-bearing capacity—in existing prestressed concrete continuous box-girder bridges with large cantilevers and thin webs, this study employed field inspections, static and dynamic load tests, and numerical simulations. Longitudinal frame models, transverse solid models, and refined interface models were developed to systematically investigate the effects of prestress loss, vehicle live loads, and temperature on crack formation. Furthermore, the effectiveness of a combined strengthening strategy involving web cross-section enlargement and internal prestressing was evaluated, with particular emphasis on the transfer efficiency of the added prestress across the interface. The results indicate that long-term prestress loss reduces the compressive stress reserve in the box-girder section and is a primary contributor to transverse cracking at the girder bottom, whereas inclined web cracking is primarily caused by the combined effects of shear stress and vertical tensile stress. Eccentric vehicle loading has a pronounced effect on the vertical tensile stress in the web; at the mid-span section, the maximum vertical tensile stress on the inner web face reached 4.24 MPa, of which 2.23 MPa was attributable to eccentric loading. After implementation of the combined strengthening strategy, the bottom-edge stress at the mid-span section decreased from 4.40 MPa to 1.74 MPa, representing a 60.45% reduction, while the mid-span deflection decreased from 30.6 mm to 20.13 mm, corresponding to a 24.54% reduction. In addition, the shear safety factor at the support increased from 0.78 to 1.10, demonstrating substantial improvements in crack resistance and overall structural stiffness. Finally, the interface stress-transfer efficiency reduction in the added internal prestress was 12.87%, indicating that the effect of interface transfer efficiency on the actual strengthening performance should be fully considered when applying the combined cross-section enlargement and internal prestressing method.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Lessons from time-dependent deflection in record span prestressed concrete bridgesScientific Reports · 2025
- Finite Element Numerical Analysis of Mechanical Performance for Continuous Rigid Frame BridgesStavební obzor · 2026
- Global Structural Performance and Repeated-Loading Effects of Steel-Concrete Composite Bridge Decks with Permanent Flat Steel Bottom Formwork.Materials (Basel, Switzerland) · 2026
- Effect of Shear Redistribution on Local Shear Buckling in Non-Prismatic Cantilever Composite Girders with Corrugated Steel WebsBuildings · 2026
- Influence of Shear Deformation on the Distortion Effect of Corrugated Steel Web Box GirdersEngineering Research Express · 2026
- A Prestress Loss Inverse Analysis Method for Long-Span PC Girder Bridges Combining Finite Element Analysis and Machine LearningEngineering Research Express · 2026