Bond Performance of Four Universal Adhesive Systems on Sound and Biomimetically Remineralized Artificially Caries-Affected Dentin Before and After Artificial Aging
Rosário Costa, Sofia Arantes-Oliveira, João Cardoso Ferreira, Álvaro Azevedo, Paulo Melo
Key points
From the paper's conclusion- Background: This study evaluated the bonding performance of four universal adhesive systems applied to sound dentin (SD) and artificially caries-affected dentin subjected to biomimetic remineralization with casein phosphopeptide–amorphous calcium phosphate (CPP–ACP), before and after artificial aging.
Abstract
Background: This study evaluated the bonding performance of four universal adhesive systems applied to sound dentin (SD) and artificially caries-affected dentin subjected to biomimetic remineralization with casein phosphopeptide–amorphous calcium phosphate (CPP–ACP), before and after artificial aging. Methods: One hundred and four human molars were allocated according to dentin substrate (SD or biomimetically remineralized [BRD]), adhesive system (FuturaBond® M+, Scotchbond™ Universal, Prime&Bond Active®, and One Coat7 Universal®), and aging (24 h or 10,000 thermocycles). Artificially caries-affected dentin was produced by pH cycling and subsequently remineralized with CPP–ACP. Adhesive interface morphology was assessed by FEG-ESEM, while shear bond strength (SBS) and failure modes were also evaluated. Statistical significance was set at p ≤ 0.05. Results: Adhesive layer thickness was significantly affected by the adhesive system, dentin substrate, and aging (p < 0.001), with a significant adhesive × substrate interaction (p < 0.001). Resin tag length was affected by the adhesive system (p = 0.03), substrate (p < 0.001), and aging (p < 0.001), with significant adhesive × substrate (p = 0.03) and adhesive × substrate × aging interactions (p = 0.001). SBS was significantly higher on SD than on BRD (p < 0.001) and decreased after thermocycling (p < 0.001). Conclusions: Universal adhesives exhibited substrate- and aging-dependent behaviour. BRD showed lower SBS than SD, while morphological differences did not consistently correspond to higher bond strength. Further studies including untreated artificially caries-affected dentin are needed to determine the specific contribution of CPP–ACP remineralization.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Microtensile bond strength and dentin–adhesive interface of universal adhesives before and after artificial aging: an in vitro studyScientific Reports · 2026
- The Use of Bovine Teeth as an Experimental Substrate in the Evaluation of Shear in Contemporary Adhesive Systems.Polymers · 2026
- Adhesive Performance of Ion-Releasing Materials on Dentin with Altered Mineralization.Journal of functional biomaterials · 2026
- Effect of incorporating chitosan/hydroxyapatite composite nanoparticles into a universal adhesive on bonding efficacy to caries-affected dentin and bioactivityBMC Oral Health · 2026
- Influence of carbonate apatite nanoparticles incorporated into commercial dental adhesives on immediate and long-term microtensile bond strength.European journal of oral sciences · 2026
- Effects of Remineralizing Products Containing NaF, CPP-ACPF, and NovaMin on Enamel Microhardness and Bond StrengthApplied Sciences · 2026