Microstructural evolution and tribological performance of SiC-reinforced FGH95 superalloy composites fabricated by spark plasma sintering
Pham Van Trinh, Nguyen Binh An, Tran Van Hau, Nguyen Duy Trinh, Tran Bao Trung, Doan Dinh Phuong
Key points
From the paper's conclusion- FGH95–SiC composites containing 2.5–10 vol% SiC were fabricated by high-energy ball milling followed by spark plasma sintering (SPS).
Abstract
FGH95–SiC composites containing 2.5–10 vol% SiC were fabricated by high-energy ball milling followed by spark plasma sintering (SPS). The effects of SiC content on the microstructure, crystallographic characteristics, hardness, and tribological behavior were systematically investigated. X-ray diffraction analysis confirmed the retention of the γ/γ′ matrix phases and SiC without detectable reaction products after SPS. The calculated γ/γ′ lattice misfit continuously decreased from 0.745% for monolithic FGH95% to 0.567% for the composite containing 10 vol% SiC, although a slight non-monotonic variation of the individual γ and γ′ lattice parameters was observed at the highest SiC content. Etched SEM observations and statistical grain-size analysis revealed only a slight decrease in average grain size from 1.15 ± 1.2 μm for FGH95 to 1.01 ± 1.0 μm for the 10 vol% SiC composite, with substantial overlap among the grain-size distributions. All specimens exhibited relative densities above 98%, indicating near-full densification, while the Vickers hardness increased from approximately 470–575 HV with increasing SiC content. Under sliding wear conditions, the wear rate decreased from approximately 5.2 × 10 −4 to 2.9 × 10 −4 mm 3 N −1 m -1 , corresponding to an improvement of approximately 45% at 10 vol% SiC. The worn-surface morphology revealed a transition from severe abrasive–delamination wear in monolithic FGH95 to predominantly mild abrasive wear in the SiC-reinforced composites. The enhanced wear resistance is primarily associated with the increased hardness and load-bearing capability of the uniformly dispersed SiC particles, together with the high densification and improved γ/γ′ crystallographic compatibility.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Balancing densification and MAX-phase stability in FAST/SPS Al–Ti₃SiC₂ compositesArchives of Civil and Mechanical Engineering · 2026
- Compositional and structural control toward boosting inner-grain prestress and releasing the inter-lattice strain of an FGH99 diffusion-bonded superalloyMaterials Horizons · 2025
- Properties of Layered Cu-Based Composites Prepared by Spark Plasma Sintering.Materials (Basel, Switzerland) · 2026
- Effect of Minor P and C Regulation on Microstructure Evolution and High-Temperature Properties of Selective Laser Melted GH4169 Superalloy.Materials (Basel, Switzerland) · 2026
- Fabrication and characterization of hybrid surface composite Al5083/Si3N4/TiC using friction stir processingJournal of Materials Research and Technology · 2026
- Characterization of Invar/Si3N4 Type Composites Obtained by Spark Plasma SinteringSilicon · 2026