Archives of Civil and Mechanical Engineering

Balancing densification and MAX-phase stability in FAST/SPS Al–Ti₃SiC₂ composites

M. Madej, A. Wąsik, M. Podsiadło, B. Leszczyńska-Madej

Key points

From the paper's conclusion
  • The results indicate that 560–580 °C represents an optimal processing window in which near-full densification is achieved while interfacial modifications remain localized, providing the most favourable combination of microstructural stability, mechanical performance and wear resistance.

Abstract

This study investigates the microstructural evolution and interfacial stability of FAST/SPS-processed Al–10 wt% Ti₃SiC₂ composites consolidated at temperatures between 500 and 600 °C. Microstructural characterization by SEM, TEM and STEM-EDS revealed progressive densification of the aluminum matrix with increasing temperature, accompanied by improved particle bonding and stable incorporation of the Ti₃SiC₂ reinforcement. The relative density increased from 92.4% at 500 °C to 99.1% at 600 °C, while hardness increased from 46 HV1 to ~ 55 HV1. TEM and STEM-EDS analyses further revealed localized interfacial features at elevated temperatures, including Ti-containing phases and local Si-rich regions near the matrix–particle interface, while the Ti₃SiC₂ reinforcement largely retained its structural integrity. Mechanical testing showed a systematic increase in compressive stress with sintering temperature, reaching ~ 525 MPa at 50% strain for the composite sintered at 600 °C. Tribological performance was strongly influenced by microstructural evolution and densification: materials processed at 500–520 °C exhibited severe adhesive-delamination wear associated with residual porosity, whereas samples sintered at 560–580 °C showed stable friction behaviour and predominantly mild abrasive wear. The results indicate that 560–580 °C represents an optimal processing window in which near-full densification is achieved while interfacial modifications remain localized, providing the most favourable combination of microstructural stability, mechanical performance and wear resistance.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers