FeSiCr/Cr2O3·SiO2·MnO soft magnetic composites constructed by interfacial reaction engineering via high-temperature oxygen release and optimization mechanistic of electromagnetic property
FENG Bo, LI Kaixuan, LI Jiang, Zhenlong Zhou, WU Zhaoyang, WANG Rui
Abstract
FeSiCr-based soft magnetic composites (SMCs) have the important applications in the field of power electronics due to the high saturation magnetization, excellent DC bias characteristics, and good environmental stability. However, the traditional insulating process struggles to balance high permeability and low loss characteristics under high-frequency and high-power conditions. To address the challenge, the interfacial reaction engineering strategy based on high-temperature oxygen release induction was proposed in this study. The MnO insulating layers with oxygen vacancies (Vo) were constructed on FeSiCr soft magnetic powders through the decomposition of manganese acetate precursor during hot-press sintering. By combining the kinetic analysis of interfacial reactions, the mechanism of Cr2O3·SiO2·MnO composite insulating layer formation via MnO−VO/FeSiCr interfacial reactions during hot-press sintering was revealed. The effect of sintering temperature (800~1100 ℃) on the microstructure evolution and magnetic properties of FeSiCr/Cr2O3·SiO2·MnO composites was systematically investigated. It is found that MnO promotes the directional oxidation of silicon and chromium at different sintering temperatures, forming the composite-structured Cr2O3·SiO2·MnO insulating layers. This unique interfacial structure enables the composites to exhibit the low loss (1282.3 kW·m−3), high permeability (32.9), high saturation magnetization (190.7 emu·g−1), and permeability stability (71% @ 65 Oe) at 30 mT and 500 kHz.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Effects of Forming Processes on Interparticle Insulation and High-Frequency Magnetic Loss of FeSi Soft Magnetic CompositesMaterials · 2026
- High-frequency FeSiAl-based soft magnetic composites via simultaneously suppressed eddy and hysteresis lossesNature Communications · 2025
- Effect of Annealing Atmosphere on the Microstructure and High-Frequency Magnetic Properties of FeSiCr Soft Magnetic CompositesMagnetochemistry · 2026
- Spatial Distribution and Local Coordination Regulation of Nano-Oxide-Modified Si-O Interfaces in FeSiAl Soft Magnetic Composites.Materials (Basel, Switzerland) · 2026
- Recent advances in hot-press sintered FeSi-based soft magnetic compositesJournal of Materials Research and Technology · 2026
- Interface microstructure and electromagnetic properties of phosphorylated FeSiB@Fe3O4 amorphous soft magnetic composites via thermal decompositionCeramics International · 2025