Key points
From the paper's conclusion- CA materials undergo clinically relevant degradation during use, particularly in TPU-based and DPAs aligners. Clinicians may need to prioritise material-specific protocols, reinforce dietary and cleaning instructions, and consider force decay when determining aligner replacement intervals. PROSPERO number: CRD420251110248.
Abstract
BACKGROUND: Clear aligner (CA) therapy has experienced rapid use over the past two decades to treat orthodontic malocclusions. However, evidence on CA material degradation in the oral environment remains limited and often focuses on single brands or isolated material properties. OBJECTIVES: To investigate CA ageing characteristics across different materials and brands and evaluate the chemical, physical, mechanical, and morphological changes following simulated or intraoral ageing. SEARCH METHODS: Five databases (PubMed, Web of Science, MEDLINE [Ovid], ProQuest, and Scopus) were searched to 18 March 2026, with no restrictions. ELIGIBILITY CRITERIA: Studies assessing CA properties after intraoral use or simulated ageing (thermocycling, cyclic loading, or liquid immersion) were included. DATA COLLECTION AND ANALYSIS: Study selection followed PRISMA 2020. RoB was assessed using QUIN for purely in vitro studies, JBI for cohort in vivo studies, and Cochrane RoB 2 for RCTs. Results were synthesised narratively and organised by property domain, as substantial methodological heterogeneity precluded formal meta-analysis. Where protocols were comparable, a simple pooled weighted mean was calculated and presented graphically. RESULTS: Ninety-five studies were included. RoB was low in eight studies, moderate in sixty-two, and high in twenty-five. Chemical composition remained largely stable during ageing, though some brands showed trace elemental release. Physical, mechanical, and morphological properties showed material-dependent deterioration. Pooled discolouration was greatest with coffee (weighted mean ΔE = 70.9), versus tea (ΔE = 18.4) and red wine (ΔE = 11.5), with Invisalign® consistently exceeding the clinically perceptible threshold. Force decay of 40-90% typically occurred within 48 h. Thermoplastic polyurethane (TPU)-based and directly printed aligners (DPAs) generally showed greater susceptibility than polyethylene terephthalate glycol-modified (PETG)-based aligners, though findings on hardness, roughness, and stiffness were inconsistent. CONCLUSIONS: CA materials undergo clinically relevant degradation during use, particularly in TPU-based and DPAs aligners. Clinicians may need to prioritise material-specific protocols, reinforce dietary and cleaning instructions, and consider force decay when determining aligner replacement intervals. PROSPERO number: CRD420251110248.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Effects of intraoral ageing on the mechanical and surface properties of clear aligner materials: A systematic review.International orthodontics · 2026
- Effects of cleaning protocols on the material properties of clear aligners and retainers: A systematic review.Journal of dental sciences · 2026
- Evaluating chemical and surface stability of thermoformed and 3D-printed clear aligners after intraoral exposurePLoS ONE · 2026
- From Polyethylene Terephthalate Glycol (PETG) to 3D-Printed Resins: A Systematic Review and Meta-Analysis of Clear Aligner Material Performance and Safety.Cureus · 2026
- Comparison of three dental resins for 3D printing of orthodontic appliances: Comparison of leaching, biocompatibility, and thermo-mechanical properties after post-curing and agingDental Materials · 2025
- Leaching and cytotoxicity of orthodontic aligner materials following simulated mechanical loading and immersion aging: An in-vitro evaluation.International orthodontics · 2026