Comparison of Flexural Strength and Flexural Modulus of Conventional and Graphene-Reinforced Polymethyl-Methacrylate under Thermocycled and Non-Thermocycled Conditions: An in-Vitro Study.
Wajiha Zia, Naseer Ahmed, Huda Adil, Rizwan Jouhar
Wajiha Zia, Postgraduate Resident, Department of Prosthodontics, Altamash Institute of Dental Medicine, Karachi, Pakistan. · Naseer Ahmed, Professor, Department of Prosthodontics, Altamash Institute of Dental Medicine, Karachi, Pakistan.
Key points
From the paper's conclusion- G-PMMA demonstrated significantly improved flexural strength and modulus compared to conventional PMMA. Thermocycling had no significant effect on flexural strength but influenced flexural modulus, indicating its impact on material stiffness rather than strength.
Abstract
BACKGROUND AND OBJECTIVE: Polymethyl methacrylate (PMMA) is widely used as a denture base material, but its major disadvantage is its low flexural strength. Graphene has recently been proposed as a reinforcing nanofiller due to its superior mechanical properties, but evidence regarding its incorporation into PMMA and the influence of thermocycling remains limited. This study aimed to evaluate the effect of graphene reinforcement on the flexural strength (FS) and flexural modulus (FM) of PMMA and to assess the impact of thermocycling on these properties. METHODOLOGY: Seventy-six PMMA samples were fabricated and divided into two groups: conventional PMMA (n = 38) and G-PMMA reinforced with 0.25 wt% graphene (n = 38). Each group was further subdivided into thermocycled and non-thermocycled groups (n=19). All samples were subjected to three-point bending tests using a universal testing machine (UTM). Data was analyzed using a two-way ANOVA followed by Bonferroni correction. (p < 0.05). RESULTS: G-PMMA displayed higher mean FS and FM than conventional PMMA in both thermocycled and non-thermocycled groups. Anova showed a statistically significant difference in flexural strength after thermocycling between PMMA and G-PMMA (p = 0.04), and for flexural modulus, PMMA vs G-PMMA, thermocycling, and their interaction had significant effects (p = 0.043, p = 0.016, and p < 0.001, respectively). Followed by pairwise comparisons, which revealed a statistically significant difference on FS between PMMA and G-PMMA after thermocycling. (p = 0.03). CONCLUSION: G-PMMA demonstrated significantly improved flexural strength and modulus compared to conventional PMMA. Thermocycling had no significant effect on flexural strength but influenced flexural modulus, indicating its impact on material stiffness rather than strength.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Comparative Evaluation of Flexural and Impact Strengths of Glass Fiber- and Titanium Dioxide Nanoparticle-Reinforced Polymethyl Methacrylate Denture Base Resin: An In Vitro Study.Cureus · 2026
- Mechanical and Micromorphological Characterization of Graphene-Reinforced PMMA Bonding to Enamel and Dentin After Surface Conditioning.Journal of functional biomaterials · 2026
- Mechanical and surface properties of PMMA denture base resins fabricated by compression molding, fluid resin, milling, and 3D printing techniques.BMC oral health · 2026
- Physicomechanical properties of PMMA denture base resins reinforced with nanofibers: a systematic review and meta-analysis.Journal of applied oral science : revista FOB · 2026
- Marginal fit, internal adaptation, and thermocycling effects on the mechanical and optical properties of graphene CAD-CAM and zirconia crowns for primary molars: An in-vitro study.Journal of oral biology and craniofacial research · 2026
- Flexural strength and surface hardness in polymethyl methacrylate provisional restorative material with zirconium nanoparticles: An in vitro study.Bioinformation · 2026