Microhardness and Dry Sliding Wear Behaviour of Ultrasonically Stir-Cast Al7075 Hybrid Nano-Composites Reinforced with SiC, B4C and Al2O3
Ravi Kant Tiwari, Satnam Singh
Key points
From the paper's conclusion- A ternary nano-ceramic addition of only 3 wt.% therefore substantially improves the dry sliding wear resistance of Al7075.
Abstract
Aluminium matrix composites are increasingly used where light weight must be combined with wear resistance. Al7075 is among the most attractive matrices, offering a high strength-to-weight ratio and good fatigue resistance. Its poor resistance to dry sliding wear, however, restricts its use in components that slide against hardened steel. Five compositions were therefore fabricated by ultrasonic-assisted stir casting, cavitation breaking up clusters that stirring alone leaves intact: the unreinforced alloy (A1) and four composites (A2-A5) reinforced with 30-40 nm powders, in which 1 wt.% SiC was held constant while Al2O3 and B4C were added at 0 or 1 wt.%. All five were cast in one campaign and tested under a common protocol, so that differences reflect composition alone; as SiC is common to every reinforced casting, the series ranks the compositions rather than isolating individual phases. Microhardness was measured for all compositions as per ASTM E384 and pin-on-disc dry sliding wear (ASTM G99) was measured at 15 to 60 N over 2700 m against hardened EN31 steel. Hardness increased by 14.3%, to 157.86 ± 3.48 HV for the ternary composite A5. The specific wear rate of A5 fell far more steeply, by 65.8% at 15 N and 57.4% at 60 N relative to A1, indicating that wear resistance is not governed by bulk hardness alone: the ceramic phases carry contact load locally and stabilise a protective tribolayer. The friction coefficient fell more modestly across the series, so the reinforcement alters how material is removed rather than merely reducing traction. Image analysis showed dispersion remained imperfect, yet A5 was still the hardest and most wear-resistant: the benefit derives from the dispersed fraction, and further gains remain accessible. A ternary nano-ceramic addition of only 3 wt.% therefore substantially improves the dry sliding wear resistance of Al7075.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Ultrasonic-Assisted Stir Casting of SiO2‑Reinforced AA7075: Microstructure, Strengthening, and Wear.ACS omega · 2026
- Dry sliding wear behavior of SiC-B4C reinforced AZ80 hybrid composites fabricated through a semi-solid stir casting processJournal of Magnesium and Alloys · 2025
- Mechanical characterization and reciprocating wear analysis of AA 7075 hybrid metal matrix composite reinforced with B 4 C and BFSInternational Journal of Materials Research · 2026
- Comparative Evaluation of Single and Hybrid Reinforcements in Aluminum Matrix Composites: Effects of SiC, Si3N4 and TiO2 Content on Mechanical and Tribological PropertiesSustainability · 2026
- Dry-Sliding Friction and Wear of Powder-Metallurgy AA6061 Composites with Multiscale TiB2–SiC ReinforcementLubricants · 2026
- Nanoparticle-reinforced Aluminium Matrix Hybrid Composites: Processing and CharacterizationJournal of Environmental Nanotechnology · 2026