Effect of enamel surface pretreatment and thermocycling on shear bond strength of metallic orthodontic brackets bonded with a self-adhesive resin: An in vitro study.
Ingrid Silva De Lima, Isadora Da Silva Ximenes, Vitor Hugo Queiroz de Barros, Ranyele Elis Alexandre Rodrigues, Ketelyn Kerty Moreira de Oliveira, Vitaliano Gomes de Araújo-Neto, Anderson Gomes Forte, Tainah Oliveira Rifane,
Paulo Picanço School of Dentistry, Fortaleza, Ceará, Brazil. Electronic address: ingridlima0510@gmail.com. · Paulo Picanço School of Dentistry, Fortaleza, Ceará, Brazil. Electronic address: isadorasximenes@gmail.com.
Key points
From the paper's conclusion- Airborne-particle abrasion significantly improved bracket bond strength to intact enamel when using a self-adhesive orthodontic resin, although thermocycling reduced adhesion regardless of surface treatment.
Abstract
OBJECTIVE: This study evaluated the effect of different enamel surface treatments on the microshear bond strength and failure mode of orthodontic brackets bonded with a self-adhesive orthodontic resin before and after thermocycling. MATERIALS AND METHODS: Bovine enamel specimens were embedded in polyvinyl chloride tubes with chemically activated acrylic resin and allocated into four groups according to enamel surface treatment: self-adhesive resin (SAR), acid etching+SAR, airborne-particle abrasion+SAR, and acid etching+airborne-particle abrasion+SAR. Each group was divided into immediate and aged conditions (n=10). Acid etching was performed with 37% phosphoric acid for 30 s, and airborne-particle abrasion with 50-μm aluminium oxide for 10 s. Brackets were bonded using Ortholink One Step adhesive. Aged specimens underwent 20,000 thermal cycles (5-55°C). Microshear bond strength was measured using a universal testing machine, and failure mode was assessed with the Adhesive Remnant Index. Data were analysed using Tukey's test (α=0.05). RESULTS: Both surface treatment and thermocycling significantly influenced bond strength. In the immediate condition, air-abraded groups showed the highest bond strength (8.16-8.55MPa), significantly exceeding non-abraded groups (5.17-5.30MPa; P<0.001). After thermocycling, air-abraded groups maintained higher bond strength (5.24-5.89MPa) than the self-adhesive resin group (2.57±1.04MPa; (F(1,41)=42.68, P<0.001). Thermocycling significantly reduced bond strength in all groups (P≤0.049). Non-air-abraded groups exhibited only ARI score 0 failures, whereas air-abraded groups showed mixed failure patterns. CONCLUSION: Airborne-particle abrasion significantly improved bracket bond strength to intact enamel when using a self-adhesive orthodontic resin, although thermocycling reduced adhesion regardless of surface treatment.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Shear bond strength of new and recycled orthodontic brackets to enamel surface: an in-vitro study.Frontiers in dental medicine · 2026
- Comparative Evaluation of Shear Bond Strength of Recycled Metal and Ceramic Orthodontic Brackets Following Different Surface Treatment Methods: An In Vitro Study.Cureus · 2026
- Effect of different surface treatments on the shear bond strength of one-step and two-step universal adhesives to enamel and dentin.BMC oral health · 2026
- Shear bond strength of metal and plastic orthodontic brackets bonded to 3D‑printed UDMA provisional resin restorations after surface treatments and aging: an in vitro study.Odontology · 2026
- Evaluation of shear bond strength of orthodontic ceramic and metal brackets with zirconia: effects of adhesive systems and storage conditionsClinical Oral Investigations · 2026
- Bonding orthodontic adhesive to non-noble metal substrates: An in-vitro comparison of surface treatments and primer systems.American journal of orthodontics and dentofacial orthopedics : official publication of the American Association of Orthodontists, its constituent societies, and the American Board of Orthodontics · 2026