Subcritical Thermal Degradation of SA210 Grade A1 Ferritic–Pearlitic Steel: Microstructural Evolution, Hardness Loss, and Strength Reduction
Rio Pudjidarma Santoso, Winarto Winarto, Jaka Fajar Fatriansyah
Key points
From the paper's conclusion- To quantify this degradation trajectory, we established a stage‐resolved framework linking subcritical thermal exposure, microstructural degradation, Vickers hardness loss, and tensile strength reduction in SA210 Grade A1 boiler tube steel.
Abstract
Ferritic–pearlitic boiler tube steel undergoes progressive microstructural degradation during subcritical overheating, impairing mechanical integrity well before severe wall thinning occurs. To quantify this degradation trajectory, we established a stage‐resolved framework linking subcritical thermal exposure, microstructural degradation, Vickers hardness loss, and tensile strength reduction in SA210 Grade A1 boiler tube steel. Isothermal annealing was conducted at 600, 660, and 720°C. Holding times reached up to 100 h at 600°C and 660°C, and up to 30 h at 720°C, producing degradation states ranging from the intact as‐received condition to an advanced carbide‐degraded morphology, classified under the Toft–Marsden six‐stage scheme. Higher temperature severely compressed the degradation timeline. Reaching Stage D required 100 h at 600°C, 30 h at 660°C, and merely 1 h at 720°C. Image analysis revealed a reduction in the pearlite‐derived dark constituent area fraction from 25.44% ± 2.27% in the as‐received condition to 11.63% ± 1.55% at Stage F, tracking the dissolution and spheroidization of continuous pearlite colonies. Ferrite grain coarsening remained minor, with the ASTM grain size number shifting from G = 9.49 ± 0.04 to G = 9.16 ± 0.03. Mechanically, median hardness fell from 167.9 HV to 121.8 HV, corresponding to a 27.4% loss, alongside a 29.55% drop in mean UTS (508.02 ± 9.71 MPa to 357.92 ± 14.61 MPa). A temperature–logarithmic time regression modeled the hardness loss with R 2 = 0.965, indicating that a 60°C thermal increment produced a softening effect equivalent to a tenfold increase in dwelling time. Relative UTS loss scaled proportionally with relative hardness loss, following ΔUTS (%) = 0.989Δ H (%) − 0.194, with R 2 = 0.962. When integrated with metallographic staging and thermal history, hardness testing serves as a robust quantitative proxy for nondestructive strength assessment in degraded boiler tubes.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Microstructure and mechanical properties of P91 welded joints after 43766 h operation of deep peak regulationJournal of Physics: Conference Series · 2026
- Study on Strength–Toughness Properties and Microscopic Fracture Mechanism of 1.4 GPa–Grade Quenched‐Partitioned and Austempered Ductile Ironsteel research international · 2026
- AE Criteria for the Loss of Load‐Bearing Capacity of Prestressing Bars After Thermal Exposure–Microstructural ValidationStructural Control and Health Monitoring · 2026
- Thermal Cycle–Microstructure–Property Relationships in Rail Steel Heat‐Affected Zone Simulated by GleebleAdvanced Engineering Materials · 2026
- Microstructure and Property Evolution of T91 Steel under Deep Peak-Shaving Service ConditionsSAE technical papers on CD-ROM/SAE technical paper series · 2026
- Effect of thermal cycling and phase transformations on chemical life of ferritic stainless steelsCorrosion Science · 2026