Microstructure and mechanical properties of P91 welded joints after 43766 h operation of deep peak regulation
Linye Zhu, Shusen Hu
Key points
From the paper's conclusion- The results reveal that severe over-tempering occurs in the LB zone, where the original martensitic lath structure completely disappears.
Abstract
Thermal power units are required to operate under deep peak regulation (DPR) to encourage the consumption of renewable energy. In this work, submerged arc welding (SAW) joints and base metal of a P91 main steam pipeline with 43,766 total operating hours and frequent long-term start-stop cycles were selected as research materials. Metallographic characterization, microhardness tests, and room-temperature and high-temperature tensile tests were carried out to systematically investigate the zonal degradation of microstructure and mechanical properties in the weld metal, low-hardness base metal (LB) zone, and high-hardness base metal (HB) zone. Comparative analysis was performed against existing data of P91 pipelines operated under steady-state service conditions. The results reveal that severe over-tempering occurs in the LB zone, where the original martensitic lath structure completely disappears. The average Vickers hardness of LB is only 170 HV, while the hardness of HB decreases to 218 HV, corresponding to a hardness reduction of 22%. The hardness discrepancy between LB and HB is far more significant than that observed in steady-state units with identical service time. The tensile strength at both room and elevated temperatures follows the sequence: high-hardness base metal > low-hardness base metal > weld metal. The LB zone possesses the lowest tensile strength reserve at all test temperatures, which is identified as the weakest zone of the pipeline. Material degradation laws established based on steady-state operating conditions cannot be directly applied to units undertaking deep peak regulation tasks. For base-metal zones with pre-existing softening induced by improper post-weld heat treatment, deep-peak-regulation cyclic thermal loading further aggravates microstructural deterioration, which remarkably elevates the premature failure risk of high-temperature pipelines during long-term service. This study provides experimental fundamentals for in-service metal monitoring and remaining service life evaluation of high-temperature pipelines in deep peak-regulation thermal power units.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Microstructure and Property Evolution of T91 Steel under Deep Peak-Shaving Service ConditionsSAE technical papers on CD-ROM/SAE technical paper series · 2026
- Insights into microstructure and mechanical integrity of P91 steel pipe repaired by temper bead welding using GTAW and SMAWDiscover Materials · 2026
- Structural Integrity of Welded Pipe Joints Made of Creep–Resistant Steel P91 with Multiple Defects: Experimental Characterization and Engineering Critical AssessmentMetals · 2026
- Microstructural and mechanical insights into friction stir welded P91 steel pipes for power plant applicationsDiscover Mechanical Engineering · 2026
- Characterization of Room and Elevated Temperature Mechanical Properties of P22/P91 Weld Metals Using Small Punch Tensile and Uniaxial Tensile Tests.Materials (Basel, Switzerland) · 2026
- Effect of Welding Thermal Cycling on the Morphology of Dislocations and Carbides in the Subcritical Heat-Affected Zone of X70 High Deformation Pipeline SteelMetals · 2026