Effect of Superabsorbent Polymer on the Properties of Fly Ash and GGBS Blended Binder Geopolymer Mortar
Renuka Senthil Muthalvan, K. Bavithra Devi, Siva Avudaiappan, Paul O. Awoyera, Olaolu George Fadugba, Erick Saavedra Flores, Nelson Maureira-Carsalade
Key points
From the paper's conclusion- This study investigates the influence of superabsorbent polymer (SAP) on the performance of FA–GGBS (30:70) blended GP mortar.
Abstract
Geopolymer (GP) mortar, synthesised through the alkali activation of fly ash (FA) and ground granulated blast furnace slag (GGBS), is considered a sustainable alternative to conventional cement‐based materials. However, its application under ambient curing conditions is often limited by shrinkage and durability‐related challenges. This study investigates the influence of superabsorbent polymer (SAP) on the performance of FA–GGBS (30:70) blended GP mortar. The blended binder was activated using a 5 M sodium hydroxide solution (SHS) and commercial sodium silicate solution (SSS), with the alkaline activator proportioned based on a sodium hydroxide flakes‐to‐SSS (SHF:SSS) mass ratio of 1:2. The SAP was incorporated at dosages ranging from 0.05% to 0.2% by weight of the binder to evaluate its influence on the fresh and hardened properties of GP mortar. Owing to its water absorption and gradual release characteristics, SAP acts as an internal curing (IC) agent that mitigates self‐desiccation shrinkage and enhances resistance to aggressive environments such as acid and sulphate exposure. However, increasing the SAP dosage resulted in a reduction in uniaxial compressive strength, which may be attributed to the additional voids formed after water release from the SAP particles. The incorporation of 0.05% SAP resulted in only a 6.8% reduction in 28‐day uniaxial compressive strength compared to the control mix, whereas acid‐induced strength loss was reduced by ~25%, demonstrating a favourable balance between mechanical performance and durability. Higher SAP dosages (0.15%–0.20%) further improved resistance to acid and sulphate attack by reducing weight loss and strength under ambient curing conditions. Qualitative SEM observations indicated the presence of SAP‐related voids, while the overall experimental results suggest that the IC effect of SAP enhanced durability despite the reduction in compressive strength at higher dosages. Overall, SAP incorporation exhibited a trade‐off between strength and durability, with 0.05% SAP providing the optimum balance from sustainable GP mortar applications.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Performance evaluation of superplasticizers in one part geopolymer mortarScientific Reports · 2026
- Fresh, Mechanical, and Durability Performance of Ambient-Cured Fly Ash-Ground Granulated Blast Furnace Slag Geopolymer Concrete: Effect of Mix Design Parameters.Materials (Basel, Switzerland) · 2026
- Role of metakaolin, alccofine, and silica fume as supplementary cementitious materials in improving durability performance of self‐compacting geopolymer concreteStructural Concrete · 2026
- Synthesis of ambient-cured geopolymer with recycled glass as binder and fine aggregate: Enhancing mechanical and durability performanceConstruction and Building Materials · 2025
- Development of Alkali-Activated Phosphogypsum Mortar Incorporating Silica Fume and Metakaolin for Enhanced Durability and CO 2 MineralisationIOP Conference Series: Earth and Environmental Science · 2026
- Development and performance of ambient cured geopolymer concrete with low alkali activation for sustainable constructionCase Studies in Construction Materials · 2026