Clinical performance of ultratranslucent monolithic zirconia posterior crowns compared with lithium disilicate crowns: A pilot, randomized, double-blind, controlled clinical trial.
Larissa Mendonça Miranda, Isabelle Helena Gurgel de Carvalho, Lidya Nara Marques de Araújo, Mutlu Özcan, Rodrigo Othávio de Assunção E Souza
Department of Dentistry, Federal University of Rio Grande do Norte (UFRN), Natal, Brazil. · Dental Materials Unit, Center for Dental and Oral Medicine, Clinic for Fixed and Removable Prosthodontics and Dental Materials Science, University of Zurich, Zentrum für Zahnmedizin, Zurich, Switzerland.
Key points
From the paper's conclusion- Both materials, ultratranslucent monolithic zirconia and lithium disilicate, demonstrated high survival rates and satisfactory clinical performance after 24 months.
Abstract
PURPOSE: To evaluate, through a pilot, randomized, double-blind, controlled clinical trial, the clinical performance of ultratranslucent monolithic zirconia (UTZr) compared to lithium disilicate (LD) posterior crowns after 24 months of follow-up. MATERIALS AND METHODS: Twenty-four crowns were fabricated and placed in 18 patients, assigned to 2 groups: Control (LD-IPS e.max CAD/Ivoclar) and Experimental (UTZr-Zircon FitPlus/Talmax). Longevity was assessed using the modified United States Public Health Service (USPHS) Ryge criteria, visual analog scales (VAS) for patients' self-perceived esthetics, and the Oral Impacts on Daily Performances (OIDP) index for quality-of-life evaluation. Evaluations were conducted at baseline (T0) and 1 (T1), 6 (T2), 12 (T3), and 24 (T4) months after cementation. Survival analysis was performed using the Kaplan-Meier method with log-rank test (α = .05). OIDP and USPHS data were analyzed descriptively, while VAS esthetic satisfaction was analyzed using Mann-Whitney, Friedman, and Wilcoxon post-hoc tests. RESULTS: The mean age of participants was 38.5 years. Eleven crowns were fabricated with LD and 13 with UTZr. After 24 months, the cumulative survival rate was 100% for both groups. Both groups showed a significant improvement in esthetic satisfaction over time (P<.05). No ceramic fractures, occlusal changes, marginal integrity alterations, or secondary caries were observed; however, one UTZr crown presented minor marginal discoloration. CONCLUSIONS: Both materials, ultratranslucent monolithic zirconia and lithium disilicate, demonstrated high survival rates and satisfactory clinical performance after 24 months.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Monolithic Zirconia Versus Porcelain-Fused-to-Metal Implant-Supported Fixed Dental Prostheses in the Posterior Region: 3-Year Results of a Randomized Controlled Clinical Trial.Clinical oral implants research · 2026
- Clinical Evaluation of CAD/CAM All-Ceramic Crowns: A Randomized Controlled Study Comparing Lithium Disilicate and Lithium Aluminosilicate.Journal of esthetic and restorative dentistry : official publication of the American Academy of Esthetic Dentistry ... [et al.] · 2026
- Clinical performance of CAD/CAM-fabricated lithium-disilicate-based glass ceramic vs. multilayer zirconia crowns after a minimum observation period of two years.Dental materials : official publication of the Academy of Dental Materials · 2026
- Randomized Controlled Clinical Trial Comparing Screw-Retained Monolithic Zirconia Implant Crowns on Standardized Titanium Base Versus Customized Titanium Abutments- 3-Years Data.Clinical oral implants research · 2026
- Evaluation of full-veneer crowns fabricated with 3D printing resin material for definitive prostheses: A 1-year randomized controlled prospective study.Journal of dentistry · 2026
- Long‐Term Clinical, Radiographic and Esthetic Outcomes of Zirconia Dental Implants: A 10‐Year Prospective Multicenter StudyClinical Oral Implants Research · 2026