From the paper's conclusion- CVD‐layer cracks reduced the strength to 42.21 ± 5.22 MPa and 41.69 ± 4.16 MPa at the waist and 45° positions, respectively, revealing that cracks in the outer CVD layer significantly degrade the C‐ring strength of bilayer tubes, while the influence of crack location (waist and 45° positions) is relatively slight.
Abstract
Defect tolerance of bilayer SiC f /SiC composite cladding tubes under C‐ring loading was evaluated by introducing laser‐machined crack‐like defects at the waist and 45° angular positions. Two crack depths were designed: cracks confined within the outer CVD‐SiC layer and cracks penetrating into the inner SiC f /SiC layer. C‐ring tests, crack‐path characterization, and finite‐element analysis were combined to reveal the depth‐position coupling effect. The uncracked tubes exhibited a nominal hoop strength of 167.88 ± 6.38 MPa. CVD‐layer cracks reduced the strength to 42.21 ± 5.22 MPa and 41.69 ± 4.16 MPa at the waist and 45° positions, respectively, revealing that cracks in the outer CVD layer significantly degrade the C‐ring strength of bilayer tubes, while the influence of crack location (waist and 45° positions) is relatively slight. When cracks penetrated into the SiC f /SiC layer, the strength further decreased to 30.60 ± 3.76 MPa and 25.86 ± 2.61 MPa. The 45° SiC f /SiC‐layer crack produced the most severe degradation, mainly owing to enhanced crack‐tip stress concentration and restricted crack deflection, interfacial debonding, and fiber pull‐out.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Effect of Steam Oxidation on Microstructure and Hoop Strength of Duplex SiC f /SiC TubeJournal of the American Ceramic Society · 2026
- Governing mechanisms of 2.5D/3D preform architectures on the microstructure, mechanical and ablation behaviors of C/C-SiC-ZrC compositesMaterials & Design · 2025
- Compressive Stress-Assisted Drilling for Delamination Suppression in C/SiC Composites: Mechanism and Experimental Validation.Materials (Basel, Switzerland) · 2026
- Out‐of‐plane Tensile Testing and Size‐Dependent Transition in Failure Mechanisms of Thin 2.5D Woven CMCsJournal of the American Ceramic Society · 2026
- Slurry Carbon–Driven Pore Evolution, Infiltration, and Mechanical Properties of Continuous Carbon Fiber‐Reinforced Silicon Carbide Composites Prepared by Slurry Impregnation Combined With Reaction Melt InfiltrationJournal of the American Ceramic Society · 2026
- C/C‐ZrC‐TiC‐SiC Composite Prepared by Joint Process of SI and RMI: Microstructure and Ablation BehaviorJournal of the American Ceramic Society · 2026