Journal of the American Ceramic Society

Effect of Steam Oxidation on Microstructure and Hoop Strength of Duplex SiC f /SiC Tube

Jia‐Pei Chen, Ze‐Xi Zhang, Gan Huang, Xin‐Zhuang Yang, Chuang‐Tian Zhan, Kun‐Heng Huang, Li‐Xiang Wu, Wei‐Ming Guo,

Key points

From the paper's conclusion
  • This study investigates the temperature‐dependent steam oxidation behavior and hoop strength degradation of silicon carbide fiber‐reinforced silicon carbide (SiC f /SiC) tube exposed to steam at 600, 900, and 1200°C for 10 days.

Abstract

This study investigates the temperature‐dependent steam oxidation behavior and hoop strength degradation of silicon carbide fiber‐reinforced silicon carbide (SiC f /SiC) tube exposed to steam at 600, 900, and 1200°C for 10 days. Site‐specific post‐test characterization was combined with mechanical testing to establish the relationship between oxidation‐induced damage and mechanical degradation. The results demonstrate that the strength degradation is non‐monotonic with temperature and is controlled by different damage mechanisms at different temperatures. At 600°C, oxidation of the PyC interphase caused void formation and local debonding of the CVD‐SiC layer, reducing the hoop strength by 44.1% to 80.5 ± 2.6 MPa. At 900°C, severe fiber‐surface damage, pit formation, and loss of distinct fiber boundaries suppressed the characteristic nonlinear deformation and progressive failure behavior, resulting in brittle fracture and the largest strength degradation of 66.8%, with a residual strength of 48.3 ± 7.5 MPa. At 1200°C, the formation of a Si‐O‐Si‐rich silica‐like oxide layer enhanced interlayer bonding, whereas gaseous oxidation byproducts generated internal voids and compromised SiC f /SiCtube integrity. Consequently, the strength degradation decreased to 50.1%, and the residual hoop strength increased to 72.6 ± 7.6 MPa. These findings indicate that the mechanical response of SiC f /SiC tube under steam exposure is governed by the competition between interfacial oxidation, fiber‐level damage, and oxide‐layer formation, rather than by temperature alone.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers

Effect of Steam Oxidation on Microstructure and Hoop Strength of Duplex SiC f /SiC Tube — Science Skim