Calcination Parameters in Laterite‐Derived Geopolymers: Reaction Kinetics, Mechanical, and Microstructural Evolution
Rodrigue Cyriaque Kaze, Özgür Cengiz, Abdolhossein Naghizadeh, Hakan Güngüneş, Gisèle Laure Lecomte‐Nana, Chaouche Mohend
Key points
From the paper's conclusion- The results identified 7.5°C/min as the optimal heating rate for crafting geopolymers with superior mechanical and microstructural attributes.
Abstract
Calcined laterite offers a promising alternative to traditional precursors in geopolymer synthesis. Despite its potential, knowledge regarding the effects of calcination conditions, particularly the heating rate, on its properties remains sparse. This research delved into the impact of different calcination heating rates on laterite and the subsequent geopolymer products by calcining laterite at 600°C for 4 h, with heating rates ranging from 1.5 to 10°C/min. Analytical techniques, including isothermal conduction calorimetry (ICC), setting time determination, XRD, TG/DTA, XF, FTIR, Mössbauer spectroscopy, ESR, and SEM/EDS, were employed to characterize both raw and calcined laterite as well as the resulting geopolymer products. This trend indicates that increasing the heating rate during thermal activation at 600°C enhanced the reactivity and dissolution behavior of the calcined laterite powder. This reduction is directly associated with heightened reaction activity and increased heat release, as noted from ICC results. Notably, mechanical properties improved at a heating rate of 7.5°C/min, giving a compressive strength of 51 MPa. The mentioned heating rate also resulted in the best porosity and water absorption values of 14% and 8%, respectively, suggestive of a more consolidated microstructure. The results identified 7.5°C/min as the optimal heating rate for crafting geopolymers with superior mechanical and microstructural attributes. Mössbauer spectroscopy revealed details of the iron site geometry and oxidation state, showing an increase in Fe 3+ content within the silicoaluminate phases. This effect was slightly more pronounced in samples synthesized with a heating rate of 7.5°C/min.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Effect of Combined Curing Regime on the Mechanical and Physical Properties of Metakaolin Based Geopolymer MortarIOP Conference Series: Earth and Environmental Science · 2026
- Calcination Effects on 3D-Printed Phosphate-Activated Geopolymer Lattices: Structure, Strength, and Stability in Acidic Media.ACS omega · 2026
- Improving the thermal stability of fly ash-based geopolymer materials through cellulose nanocrystal reinforcementJournal of Materials Science · 2025
- Sustainable Geopolymer Mortars from Ceramic Sanitaryware Waste: Impact of Curing Methods on Mechanical and Thermal BehaviorMaterials · 2026
- Understanding microstructure evolution of cast geopolymers based on metakaolin and ceramic tile wasteCeramics International · 2026
- Refractory Metakaolin Geopolymers: Achieving High Mechanical Strength and Near‐Zero Shrinkage After Exposure to 800°CJournal of the American Ceramic Society · 2026