Sustainable Geopolymer Mortars from Ceramic Sanitaryware Waste: Impact of Curing Methods on Mechanical and Thermal Behavior
Rim Benkabou, Abir Rezzoug, Kada Ayed, Aïssa Asroun, Zouaoui R. Harrat, Mohammed Chatbi, Ercan Işık, Fatih Avcil,
Université Djilali de Sidi Bel Abbès · Polytechnic School of Algiers
Key points
From the paper's conclusion- Microstructural characterization using scanning electron microscopy coupled with energy-dispersive spectroscopy and X-ray diffraction supported the observed mechanical trends under different curing conditions.
Abstract
This study investigates the influence of curing conditions on mechanical performance, residual strength after high-temperature exposure, and microstructural evolution of geopolymer mortars based on ceramic sanitaryware waste (CSW). Direct and delayed thermal curing regimes were applied at 60 °C and 80 °C for 48 h and 72 h. The fresh mixtures exhibited adequate workability with a flow diameter of 21 cm, indicating suitable consistency for casting. Results show that direct curing consistently enhances compressive strength, reaching 30.97 MPa at 80 °C for 72 h, compared with 15.88 MPa under delayed curing. Increasing curing temperature and duration improved early-age mechanical performance, particularly under direct curing conditions. After exposure to 800 °C, directly cured specimens retained higher residual compressive strength, with an improvement of approximately 6.6% compared with delayed-cured specimens. Microstructural characterization using scanning electron microscopy coupled with energy-dispersive spectroscopy and X-ray diffraction supported the observed mechanical trends under different curing conditions. The findings highlight the role of curing strategy in optimizing CSW-based geopolymer mortars for construction applications where mechanical performance and high-temperature resistance are required.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- High-Temperature Behavior and Mechanical Performance of Ceramic Brick and Metakaolin Waste Based-Geopolymer Binder.Materials (Basel, Switzerland) · 2026
- Effect of Combined Curing Regime on the Mechanical and Physical Properties of Metakaolin Based Geopolymer MortarIOP Conference Series: Earth and Environmental Science · 2026
- Thermal performance of brick masonry bonded by cement/geopolymer mortar: efficiency of built and repairingJournal of Thermal Analysis and Calorimetry · 2025
- Physical and microstructural characterization of wood ash–based geopolymer mortars with ceramic powder under different curing regimesConstruction and Building Materials · 2025
- Understanding microstructure evolution of cast geopolymers based on metakaolin and ceramic tile wasteCeramics International · 2026
- Mechanical and Residual Performance of Fly Ash-Based Geopolymer Mortars Incorporating Recycled Brick-Tile/Ceramic Aggregates and Polypropylene Fibers.Polymers · 2026