Microstructure and Grinding Performance of Resin‐Bonded Agglomerated Abrasives From KH550‐Modified Brown Fused Alumina
Zhe Qiao, Zhengxin Li, Guowei Zhang, Xue Liu, Pengyu Yang
Key points
From the paper's conclusion- Brown fused alumina (BFA) abrasives were surface‐modified with γ‐aminopropyltriethoxysilane (KH550) at 0–2.0 wt% and used to fabricate resin‐bonded agglomerated abrasives and abrasive cloths.
Abstract
Brown fused alumina (BFA) abrasives were surface‐modified with γ‐aminopropyltriethoxysilane (KH550) at 0–2.0 wt% and used to fabricate resin‐bonded agglomerated abrasives and abrasive cloths. The modified abrasives were characterized by FTIR, SEM‐EDS, and XPS, and agglomerate abrasive granules were evaluated for morphology, bulk density, and single‐particle compressive strength. Grinding performance was assessed via grinding ratio, efficiency, force, and temperature. Results showed that KH550 bonded to BFA via Si–O–Al linkages, with XPS confirming a monolayer structure (Si/N = 1.31). For agglomerated abrasives modified with 0.5–1.0 wt% KH550, resin wetting improved, increasing bulk density from 0.70 to 0.75 g/cm 3 and compressive strength from 83 to 91–92 N. At ≥1.5 wt%, excess silanol self‐condensation produced thick siloxane coatings that covered abrasive edges, degrading mechanical properties and self‐sharpening. When grinding 304 stainless steel, the 0.5 wt% modified agglomerated abrasive cloth achieved the optimal grinding performance, with a grinding ratio of 2.40 and efficiency of 5.54 g/h (increases of 62.2% and 59.2% over the unmodified specimen). Real‐time monitoring showed a low tangential force (∼24–25 N), minimal fluctuation, and a moderate grinding temperature (∼205°C), confirming synergistic optimization of interfacial bonding and self‐sharpening. The optimal dosage was also confirmed on TC4 titanium alloy.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Microstructure and Properties of CBN Abrasive Blocks with Cu-Sn-Ti Binder Modified by Ceramic Glass Powder.Materials (Basel, Switzerland) · 2026
- Experimental optimization of abrasive brush deburring for burr control in automotive manufacturingResults in Materials · 2026
- Single-Step Induction Brazing of Ceramic–Metal Hybrid Joints: Tailoring Zirconium Content for Microstructure and Mechanical PerformanceApplied Sciences · 2026
- Effect of Surface Modification on In Situ Mechanical Properties of Brazed Joints Between Porous Si 3 N 4 and TiAl AlloysJournal of the American Ceramic Society · 2026
- Effects of grain size on bonding performance of Cu-to-Cu bondingJournal of Materials Research and Technology · 2025
- Influence of Modifying Additives on Resin-Bonded Diamond Tool and Single-Crystal Silicon Lapping Performance.Materials (Basel, Switzerland) · 2026