Preparation and Corrosion Behavior of KAlSiO 4 ‐KAl 11 O 17 Composites for Synthesizing Na‐Ion Battery Cathode Materials
Meiling Xie, Lihua Zhu, Minghao Fang, Zhaohui Huang, Xin Min
Key points
From the paper's conclusion- The corrosion behavior and mechanisms of these composites were investigated using the O 3 ‐NaNi 1/3 Fe 1/3 Mn 1/3 O 2 (NNFM) cathode material precursor, which consists of Ni 1/3 Fe 1/3 Mn 1/3 (OH) 2 and Na 2 CO 3 as the corrosive medium.
Abstract
Against the backdrop of rapidly growing market demand for sodium‐ion battery (SIB) cathode materials, saggars serve as critical storage and transportation components in the cathode materials sintering process. Accordingly, developing high‐performance saggars with excellent corrosion resistance and prolonged service life is of great significance. In this work, nepheline (KAlSiO 4 ) and hexaaluminate (KAl 11 O 17 ) powders prepared by the high‐temperature solid‐state method were used as raw materials to prepare inks suitable for direct ink writing. A dual‐feed direct ink writing system was employed to fabricate KAlSiO 4 ‐KAl 11 O 17 composites with different compositions, verifying the feasibility of the 3D printing for producing composition tunable composite refractories. The corrosion behavior and mechanisms of these composites were investigated using the O 3 ‐NaNi 1/3 Fe 1/3 Mn 1/3 O 2 (NNFM) cathode material precursor, which consists of Ni 1/3 Fe 1/3 Mn 1/3 (OH) 2 and Na 2 CO 3 as the corrosive medium. After the KAlSiO 4 ‐KAl 11 O 17 composite was exposed to NNFM at 900°C for 6 h, the primary corrosion products were NaAlSiO 4 , (Na 2 O) 0.33 NaAlSiO 4 , NaAl 11 O 17 , and NaAlO 2 , with a corrosion depth of approximately 45 µm, demonstrating excellent corrosion resistance. The corrosion process of the nepheline‐hexaaluminate composite primarily involved chemical reaction dissolution and penetration diffusion mechanisms.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- In Situ Dense Interfacial Barrier via Tailored CA 6 Gradation and Si Doping for Durable Li‐Ion Battery SaggarsJournal of the American Ceramic Society · 2026
- In Situ Mullite Formation in 80 wt% Alumina Ceramics via Kaolin/Ca3(PO4)2 Ratio Modulation: Densification, Microstructural Evolution, and Dielectric Breakdown BehaviorInorganics · 2026
- Improved Phase Purity and Sodium-Ion Diffusion in Na₄ Fe₃ (PO₄ )₂ P₂ O₇ Cathodes via Carbon Source OptimizationEnergy & Fuels · 2025
- SiC-BN composites with extreme thermal and environmental stabilityarXiv · 2026
- Interaction of MgO Recyclate‐Based Cermet Anode With KF‐AlF₃ ‐Al₂ O₃ at 800°C During Laboratory Scale Aluminum Molten Salt ElectrolysisAdvanced Engineering Materials · 2026
- Boosting Long‐Life Sodium Storage of Na₄ MnV(PO₄ )₃ via Synergistic Bond Structure Regulation and Interfacial ModificationAdvanced Functional Materials · 2025