Cyclic Bond Behavior of Deformed Bars in Modified Crumb Rubber Concrete with Nano-Silica and Steel Fiber: An Experimental Study
Rajon Dey, Muhammad Iftiarul Islam, Daniyal Hadi, Syeda Tabassum, Parvez Ahamed Sojib, Oren Atobrhan Sereke, Sir Zameen
Key points
From the paper's conclusion- This experiment demonstrates the cyclic behavior of bond of deformed reinforcing bars inserted in modified crumb rubber concrete with steel-fiber and nano-silica (SFNS-CRC) under moderate repeated tensile loading, representing service-level cyclic actions where slip accumulation governs performance.
Abstract
This experiment demonstrates the cyclic behavior of bond of deformed reinforcing bars inserted in modified crumb rubber concrete with steel-fiber and nano-silica (SFNS-CRC) under moderate repeated tensile loading, representing service-level cyclic actions where slip accumulation governs performance. Ran pull-out tests using Losberg-type specimens with 150 mm size cubes and 16 mm rebar embedded centrally. The experimental matrix included two concrete grades (C35 and C45), two embedment lengths (3D and 5D respectively 48 mm and 80 mm), and two upper cyclic load levels (0.3 Pm and 0.5 Pm ), where Pm is the monotonic pull-out capacity from companion tests. The lower load was fixed at 0.1Pm, and all specimens were subjected to 200 cycles at 2 Hz before final monotonic pull-out failure. For C45 SFNS-CRC, cube compressive, splitting tensile, and axial compressive strengths were 56.13 MPa, 7.00 MPa, and 48.31 MPa, respectively. Compared with unmodified C45 crumb rubber concrete, steel fiber and nano-silica increased these strengths by 10.69%, 29.63%, and 21.63%. Under cyclic loading, hysteresis loops remained narrow and stable, while residual slip increased progressively with cycle number and load amplitude. Strain measurements showed cyclic loading shifted bond stress transfer toward deeper embedment regions & the C45 specimen with 3D embedment reached a post-cyclic ultimate bond strength of 26.748 MPa at an upper cyclic level of 0.5 Pm , compared with 26.221 MPa at 0.3 Pm , representing a difference of only 2.01%. However, increasing the upper cyclic level from 0.3 Pm to 0.5 Pm increased the peak free-end slip by 4.77%, indicating that moderate cyclic loading affected interface deformation more strongly than post-cyclic peak bond strength. Increasing concrete grade from C35 to C45 enhanced cyclic bond strength of 3D specimens by 16.39%, while increasing embedment length from 3D to 5D raised ultimate pull-out load by 36.99% but reduced nominal average bond stress by 17.81%. The normalized bond index (τu/√ fc ) ranged from 2.93 to 3.57, with the highest value obtained for the C45 specimen with 3D embedment Overall, SFNS-CRC exhibited stable cyclic bond behavior, governed mainly by residual slip accumulation and bond stress redistribution.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Microstructure-Guided Optimization of Steel Fiber-Reinforced Crumb Rubber Concrete for Sustainable and Lean ConstructionBuildings · 2026
- Bond failure of corroded rebar embedded in rubberized geopolymer concrete: Experimental evaluationConstruction and Building Materials · 2026
- Investigating the Performance of Rehabilitated Non-Prismatic Reinforced Concrete Columns Subjected to Cyclic LoadCivil and Environmental Engineering · 2026
- Bond behavior of corroded reinforcement: Experimental investigation and finite element analysisStructural Concrete · 2026
- Experimental and numerical investigation of rubberized concrete beam-column joints subjected to monotonic loading.Scientific reports · 2026
- Strength reduction of crumb rubber concrete: microstructures and mesoscale modellingInternational Journal of Mechanical Sciences · 2025