Mechanical and Thermal Behavior of Mortars Containing Waste Foundry Sand Exposed to High Temperatures
Camila Moura, Gisleiva Ferreira, Lucas Barbieri, Michelle Rodrigues, Armando Moreno, Rafaela Amaral
Key points
From the paper's conclusion- The results showed that the incorporation of up to 50% WFS did not compromise the residual mechanical performance of the mortars.
Abstract
Considering the high occurrence of fire-related accidents in buildings, there is a clear need to investigate the behavior of cementitious materials when exposed to elevated temperatures. In this context, rendering mortars deserve special attention due to their fundamental role in protecting buildings during fire events, particularly regarding the evaluation of their mechanical properties when alternative materials, such as waste products, are incorporated as substitutes for natural aggregates. Among these waste materials, Waste Foundry Sand (WFS) stands out because its physicochemical characteristics are similar to those of natural sand. However, the literature still lacks studies addressing one of the most relevant mechanical properties of rendering mortars: the static modulus of elasticity, obtained through destructive testing, and the dynamic modulus of elasticity, determined by ultrasonic testing, after exposure to high temperatures. Therefore, the objective of this study was to analyze the residual mechanical properties of rendering mortars produced with WFS and subjected to elevated temperatures. For this purpose, cylindrical specimens were manufactured with different replacement levels of natural sand by WFS (0%, 30%, 50%, and 70%). After 90 days of curing, the specimens were exposed to temperatures of 200, 400, 600, and 800 °C. Initially, ultrasonic pulse velocity tests were performed to determine wave propagation velocity and the dynamic modulus of elasticity (Ed). Subsequently, the static modulus of elasticity (E) and compressive strength were determined through destructive testing. In addition, a numerical analysis based on the finite element method was conducted to evaluate temperature distribution and isotherms within the specimens during heating. The results showed that the incorporation of up to 50% WFS did not compromise the residual mechanical performance of the mortars. Furthermore, the ultrasonic method proved to be effective in estimating the compressive strength of the mortars. The numerical analysis indicated that REF e T30 exhibited similar behavior regarding heat flow from the surface to the core of the specimens.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Mechanical and Microstructural Performance of Mortars with Ladle Furnace Slag after Thermal ExposureJournal of Physics: Conference Series · 2026
- Mechanical and Microstructural Performance of Different Plaster Mortars Used to Protect Interior Concrete Exposed to Elevated Temperatures.Polymers · 2026
- Influence of Polypropylene Fibres on Energy Dissipation Mechanisms and Thermo-Chemical Degradation of Cement Mortars Subjected to High Temperatures.Materials (Basel, Switzerland) · 2026
- Residual physio-mechanical properties and degradation analysis of foamed concrete exposed to elevated temperaturesScientific Reports · 2025
- Multiscale Evaluation of the High-Temperature Performance of Cement Mortars Containing Class C and F Fly Ash.Materials (Basel, Switzerland) · 2026
- Residual Mechanical Performance and Mass Loss of Heat-Cured NaOH-Activated Fly Ash/Slag and Portland Cement Mortars After Exposure to Elevated TemperaturesBuildings · 2026