Journal of Physics: Conference Series

Comparison of carburizing heat treatment properties of slider steel and research on hole position deformation control

Yanan Song, Kaipeng Zhao, Qingle Hao, Xiaopeng Su, Lujun Wang, Xiaofei Ren, Zhen Li, Lei Zhang

Key points

From the paper's conclusion
  • Analysis of operational condition adaptability confirms that the optimized 20CrMoH is better suited for medium-load, high-precision sliders, offering valuable engineering insights for material selection and deformation control in precision slider carburizing processes.

Abstract

To tackle engineering challenges such as the poor microstructural stability, uneven hardened layer distribution, excessive hole deformation, and ambiguous material selection adaptability encountered in the carburizing heat treatment of precision sliders, this study systematically compares the microstructural characteristics and hardened layer properties of three slider steels —20CrMoH, 20CrMnTi, and 18Cr2Ni4MoA—after undergoing carburizing, quenching, and subsequent low-temperature tempering. Furthermore, research is conducted to optimize the thermal deformation process for the hole positions in 20CrMoH sliders. The experimental findings reveal that variations in alloy composition result in significantly different strengthening effects among the three steels. Specifically, 20CrMnTi demonstrates inadequate hardenability and an abrupt hardness gradient transition; 18Cr2Ni4MoA exhibits a high residual austenite content in the surface layer, leading to compromised dimensional stability; in contrast, 20CrMoH, following carburizing, features a homogeneous and dense microstructure without notable defects, a smooth hardened layer gradient, and superior overall mechanical properties. Through single-variable experiments, the optimal low-deformation process for 20CrMoH is identified as follows: preheating at 650°C, segmented carburizing at 910°C, pre-cooling and step quenching at 810°C, and tempering at 170°C for 2 hours, which effectively controls distortion of hole spacing (∆L) deviation within 0.15 mm. Analysis of operational condition adaptability confirms that the optimized 20CrMoH is better suited for medium-load, high-precision sliders, offering valuable engineering insights for material selection and deformation control in precision slider carburizing processes.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers