Mechanism Analysis and Comprehensive Management of Hydrogen Corrosion Failure in Water Wall Tubes of a Subcritical Boiler
Ran Wei, Baocang Du, Wenqian Jiang, Xian Xu, Wei Chang, Yan Li, Qingdong Chang, Bingbing Ren,
Key points
From the paper's conclusion- This study investigates water wall tubes of a boiler that experienced multiple leakages within three months after only 24, 860 hours of service.
Abstract
Hydrogen corrosion, as a typical form of under-deposit corrosion failure, is essentially an irreversible brittle damage caused by the reaction between metallic materials and hydrogen under high-temperature and high-pressure environments. Its occurrence mechanism involves several key stages: water quality deterioration leads to scaling on the inner wall of tubes; an acidic or alkaline corrosive environment forms beneath the scale, destroying the protective film; iron reacts with water vapor to generate hydrogen atoms; hydrogen atoms diffuse into the metal along grain boundaries and react with cementite to produce methane; methane accumulates at grain boundaries, generating local high pressure, which subsequently initiates intergranular microcracks. This study investigates water wall tubes of a boiler that experienced multiple leakages within three months after only 24, 860 hours of service. Systematic failure analysis was conducted using macroscopic observation, chemical composition analysis, mechanical property testing, metallographic examination, and scale quantity and composition analysis. The results indicate that the root cause of the accident is hydrogen corrosion. Based on these findings, a comprehensive prevention and management scheme is proposed, encompassing boiler operation optimization, enhanced chemical supervision, upgraded metal inspection, and multi-department collaborative governance, aiming to provide technical references for failure prevention and life management of similar boilers.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Degradation Behavior and Optimization Strategies for Metallic Materials in High-Temperature Hydrogen Service: A Review.ACS applied materials & interfaces · 2026
- Corrosion Product Films as Natural Barriers for Hydrogen Energy Pipelines: Structure-Permeation Correlations.Small (Weinheim an der Bergstrasse, Germany) · 2026
- Hydrogen Behavior and Mechanism of Cr-Coated Zirconium Alloy Cladding During Simulated LOCA Tests.Materials (Basel, Switzerland) · 2026
- Failure Analysis of Economizer Tube Leakage Caused by Localized Internal Corrosion at Weld-Root RegionsRecent in Engineering Science and Technology · 2026
- A Study on the Service Degradation and Failure Mechanisms of Austenitic Heat-Resistant Steel Tubes in the Radiation Section of an Ethylene Cracker Furnace Based on a Multi-Evidence Diagnostic FrameworkMetals · 2026
- Hydrogen Degradation and Integrity Assessment of Cracked X80 Pipelines Under Hydrogen-Blended Natural Gas ConditionsEnergies · 2026