Hydrogen Degradation and Integrity Assessment of Cracked X80 Pipelines Under Hydrogen-Blended Natural Gas Conditions
Peifen Yao, Yaoyinqi Wang, Qiaosheng Zhang, Shengde Di, Xiaoming Luo
Key points
From the paper's conclusion- The proposed framework establishes a direct linkage between material degradation and pipeline-scale integrity assessment, providing a practical approach for safety evaluation and integrity management of defective hydrogen-blended natural gas pipelines.
Abstract
Hydrogen-blended natural gas transportation offers a cost-effective pathway for large-scale hydrogen utilization by leveraging existing natural gas pipeline infrastructure. However, hydrogen-induced degradation of pipeline steel mechanical properties and accelerated crack growth increase the failure risk of defective pipelines. Establishing the relationship between hydrogen-induced material degradation and structural integrity is therefore essential for ensuring safe pipeline operation. In this study, a hydrogen concentration-dependent degradation model was developed through experimental calibration. The evolution of X80 steel mechanical properties was incorporated into finite element models of cracked pipelines to assess structural integrity under hydrogen-blended natural gas conditions. The effects of hydrogen concentration and crack geometry on plastic limit load, crack-front J-integral distribution, and fatigue crack growth behavior were systematically investigated. The results demonstrate that hydrogen concentration is the primary factor governing plastic load-carrying capacity by reducing material strength and ductility, whereas crack geometry, particularly crack depth, dominates the fracture driving force. Compared with static fracture behavior, hydrogen concentration has a limited effect on fracture driving force but significantly accelerates fatigue crack growth and reduces fatigue life, with the most pronounced degradation occurring during the increase in low hydrogen concentrations. These findings reveal the differentiated roles of hydrogen-induced degradation in plastic collapse, static fracture, and fatigue damage mechanisms. The proposed framework establishes a direct linkage between material degradation and pipeline-scale integrity assessment, providing a practical approach for safety evaluation and integrity management of defective hydrogen-blended natural gas pipelines.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Investigation of Welded Joints of Pipelines from an Existing Gas Transmission Network Exposed to Hydrogen—Part I: Structure, Mechanical Properties and Susceptibility to Hydrogen EmbrittlementMetals · 2026
- Influence of Dual‐Crack Evolution on Fatigue Life of Hydrogen‐Transmission Welded Steel Pipelines Under Multifield CouplingFatigue & Fracture of Engineering Materials & Structures · 2026
- Experimental and Machine Learning-Based Assessment of Fatigue Crack Growth in API X60 Steel Under Hydrogen–Natural Gas Blending ConditionsMetals · 2025
- Hydrogen-Induced Damage Evolution and Quasi-Cleavage Cracking in API X70 Pipeline Girth Welds Under Blended CH4-H2 EnvironmentsCrystals · 2026
- Investigation of Welded Joints of Pipelines from an Existing Gas Transmission Network Exposed to Hydrogen—Part II: Some Aspects of the Microstructural Mechanisms of Hydrogen-Assisted Damage and FractureMetals · 2026
- Corrosion Product Films as Natural Barriers for Hydrogen Energy Pipelines: Structure-Permeation Correlations.Small (Weinheim an der Bergstrasse, Germany) · 2026