Cracking failure analysis of a natural gas pipeline
Bowen Zhang, Yongan Tang, Dan Xu, Junyi Fang, Zhujun Liu
Key points
From the paper's conclusion- Local cracking failure occurred on a natural gas transmission pipeline in Northeast China.
Abstract
Local cracking failure occurred on a natural gas transmission pipeline in Northeast China. Through the test and analysis of fracture morphology, chemical composition, metallographic structure, and mechanical properties of the pipeline, the failure mechanism is investigated. The results show that the chemical composition and mechanical properties of the pipeline cannot meet the requirements of relevant standards. The matrix exhibits a martensitic structure, with the yield strength and tensile strength reaching as high as 1182 MPa and 1401 MPa, respectively, but the elongation to fracture is only 11%, which shows both high hardness and strength but relatively low ductility, presenting high hydrogen embrittlement sensitivity. Meanwhile, high contents of C and S elements are detected in the corrosion products on the fracture surfaces. Moreover, the typical characteristic of crack propagation along the grain boundary is observed, proving the presence of H 2 S in the transmission gas. The H atoms generated by the cathode reaction (2H + + 2e − → 2H) would penetrate into the interior of the pipeline under the action of H 2 S and accumulate at the martensitic grain boundaries, reducing the bonding strength. Under the combined actions of internal pressure and bending stress, microcracks would initiate at the grain boundaries and propagate along the grain boundaries, eventually causing intergranular fracture of the pipeline.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Investigation of Welded Joints of Pipelines from an Existing Gas Transmission Network Exposed to Hydrogen—Part I: Structure, Mechanical Properties and Susceptibility to Hydrogen EmbrittlementMetals · 2026
- Investigation of Welded Joints of Pipelines from an Existing Gas Transmission Network Exposed to Hydrogen—Part II: Some Aspects of the Microstructural Mechanisms of Hydrogen-Assisted Damage and FractureMetals · 2026
- Experimental and molecular dynamics evaluation of grain size effects on hydrogen trapping and mechanical performance of pipeline steel.Journal of materials science. Metallurgy · 2026
- Root Cause Analysis of Girth Weld Cracking in a Mechanically Lined Pipeline.Materials (Basel, Switzerland) · 2026
- A multiscale study on the synergistic failure mechanism of H2S corrosion and hydrogen embrittlement of X80 pipeline steelInternational Journal of Hydrogen Energy · 2026
- Hydrogen-Induced Damage Evolution and Quasi-Cleavage Cracking in API X70 Pipeline Girth Welds Under Blended CH4-H2 EnvironmentsCrystals · 2026