  • The low-velocity impact response of hybrid glass/carbon filament-wound composite pipes with a nominal outside diameter of 24 mm was investigated experimentally, analytically and numerically.

Abstract

The low-velocity impact response of hybrid glass/carbon filament-wound composite pipes with a nominal outside diameter of 24 mm was investigated experimentally, analytically and numerically. Two radial sequences, 45G45C and 45C45G, were tested at nominal conditions of 40, 60 and 80 J (n = 3 per condition). The 80 J condition also involved a higher impactor mass and momentum. A first-order architecture-only stiffness model was used, and an Abaqus/Explicit model with continuum-shell plies and cohesive interfaces was applied only at 40 J for qualitative-to-semiquantitative interpretation. A comparative ignition-loss check yielded similar apparent retained-fiber estimates, not definitive constituent fractions. Mean peak force for 45G45C was 13.3%, 6.1% and 5.3% higher than for 45C45G at 40, 60 and 80 J, respectively; however, the sequence main effect was not statistically significant (p = 0.103). The different mean wall thicknesses (3.07 and 3.32 mm, respectively) prevent attribution to stacking sequence alone. Within this exploratory dataset, nominal impact condition was associated with peak force and displacement. The observed differences remain preliminary; numerical damage patterns are unvalidated predictions, not evidence of improved post-impact damage tolerance.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers