Structural Response of Basalt–Glass Interply Hybrid Filament‐Wound Composite Pipes Under Quasi‐Static Transverse Compression and Lateral Crushing

Özkan Özbek, İrfan Berk Efe

Key points

From the paper's conclusion
  • In conclusion, the results identify interply stacking sequence as a critical design parameter for tailoring the stiffness, deformation behavior, crushing stability, and energy absorption of filament‐wound glass–basalt composite pipes under transverse loading.

Abstract

This study experimentally investigated filament‐wound glass–basalt interply hybrid composite pipes with different stacking sequences under quasi‐static transverse loading. Eight configurations, including non‐hybrid glass and basalt pipes and their hybrid combinations, were manufactured by wet filament winding and evaluated through transverse compression and crushing tests. The results showed that both fiber type and stacking sequence strongly influenced stiffness, deformation, crushing stability, and energy absorption. The pure basalt pipe (BBB) achieved the highest pipe stiffness (13.4 MPa), corresponding to an 18% increase over the pure glass pipe (GGG), whereas the latter reached the highest first peak load and underwent greater cross‐sectional deformation. Under lateral crushing over a displacement range of 0–40 mm, the hybrid configurations generally showed greater post‐peak stability, although their performance varied considerably with ply arrangement. In particular, GGB achieved the highest mean crushing load (7.8 kN), crush force efficiency (132%), total energy absorption (312.78 J), and specific energy absorption (3.7 J/g). Multi‐scale damage observations revealed that matrix cracking, fiber fracture, fiber/matrix debonding, and interlaminar delamination interacted throughout the deformation process, with hybridization modifying the distribution and propagation of damage. Substantial differences among pipe configurations containing the same constituent fibers further demonstrated the decisive role of their through‐thickness arrangement. In conclusion, the results identify interply stacking sequence as a critical design parameter for tailoring the stiffness, deformation behavior, crushing stability, and energy absorption of filament‐wound glass–basalt composite pipes under transverse loading.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers

Structural Response of Basalt–Glass Interply Hybrid Filament‐Wound Composite Pipes Under Quasi‐Static Transverse Compression and Lateral Crushing — Science Skim