Production of 3D Printed Suture Anchoring Screw Based on Biopolymer Coated by Chitosan/HAp Using Dip Coating Method to Enhance Bioactivity
Muhamad Bahrul Ulum, Muhammad Rizky Aulia Susilo, Riska Ayu Ramadhana Putri, Adzrofil Tsabitah Basyasyah, Alfidah Nur Denya, Achmad Dwitama Karisma
Key points
From the paper's conclusion- The results of the EDX test of coating variations of samples A and C are by the Ca/P ISO 13175-3 standard with an optimal range of 1.59 - 1.72.
Abstract
A medical tool utilized in orthopedic surgery operations is the suture anchor screw. Stainless steel or titanium are the materials typically used to make suture anchors, and these materials are tough for the body to absorb. Suture anchors made of biopolymer material are, therefore, one way to solve this issue. Nevertheless, suture anchors made of biopolymer materials still have certain bioactivity issues; thus, the dip coating technique is required to address this issue. Dip coating has emerged as a highly pertinent and intriguing coating technique for additional study in the medical field. Chitosan can increase the antimicrobial activity. As hydroxyapatite, or HAp, is utilized to promote bone regeneration, it also possesses certain antibacterial properties like those of chitosan. There are three variations of hydroxyapatite mass coating in PLA 3D printing, which results in a significant difference compared to the other two variations that have no hydroxyapatite coating at all. FTIR spectroscopy can identify a substance that contains a hydroxyl group (OH - ). The substance or surface can be composed of PLA, hydroxyapatite, or chitosan. The FTIR test itself shows that there is an amine group (NH) owned by chitosan and a phosphate group (PO4) owned by HAp. The C=O cluster owned by the PLA is not visible because it is perfectly coated. The results of the EDX test of coating variations of samples A and C are by the Ca/P ISO 13175-3 standard with an optimal range of 1.59 - 1.72. In the compressive strength test, it can be said that the coating plays a very important role in the increase in compressive strength. The addition of HAp as a reinforced filler is very influential as an increase in compressive strength. The more HAp, the stronger the suture anchoring screw produced. Scaffolds with HAp solution have antibacterial activity against Staphylococcus aureus bacteria with an inhibitory zone range of 3.24 mm.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Coating Nano Hydroxyapatite Based on Rice Snail Shells (Pila ampullacea) /Chitosan/Hyaluronic Acid on Titanium (Ti-6Al-4V) Using Electrophoretic Deposition Method for Biomedical ApplicationsEPJ Web of Conferences · 2026
- Composition-Dependent Electrochemical Behavior and Preliminary Biological Screening of Hydrothermal Hydroxyapatite–Chitosan–Palladium Coatings on β-Ti30Zr5MoMaterials · 2026
- Study of the Structure and Properties of SiO2-Reinforced HA-Based Coatings Produced by Atmospheric Plasma SprayingCoatings · 2026
- Impact of chitosan addition on the characteristics and antibacterial properties of fluorapatite-copper(II) oxide synthesized via sol-gel methodPure and Applied Chemistry · 2026
- Interaction of BSA with Ta2O5 Nanoparticles: The Effect of Polydopamine Pre-CoatingMolecules · 2026
- Dual-Phase Chitosan Incorporation in Alginate/Fe(III) Hydrogel Beads: Multi-Scale Spectroscopic Evidence for Gradient-Confined Phosphate Precipitation and Implications for Adsorbent Design.Environmental research · 2026