High-affinity phosphate capture on MgO/Mg(OH)2-decorated wattle bark biochar: adsorption mechanism and regeneration performance.
Elham Jalali, Elizabeth Erasmus, Shahab Maghsoudi, Marietjie Schutte-Smith, Hendrik G Visser
Chemistry Department, University of the Free State Bloemfontein 9300 South Africa Jalali.E@ufs.ac.za visserhg@ufs.ac.za. · Department of Chemistry, Faculty of Science, Shahid Bahonar University of Kerman Kerman Iran.
Key points
From the paper's conclusion- The initial phosphate removal efficiency of MgO-BC was found to be over 80% after five adsorption-desorption cycles, which confirms good regeneration potential.
Abstract
MgO modified wattle bark biochar (MgO-BC) was produced by impregnating wattle bark with MgCl2 followed by pyrolysis at 600 °C and tested for the removal of phosphate from water. Material characterization showed the successful incorporation of MgO/Mg(OH)2 phases onto the biochar matrix and the presence of surface functionalities that are relevant for phosphate binding. Response surface methodology showed that solution pH, MgO-BC dosage, contact time, and initial phosphate concentration significantly influenced phosphate removal. The optimized conditions were pH 8.0, an MgO-BC dosage of 0.059 g in 10 mL solution, a contact time of 21 h, and an initial phosphate concentration of 64.6 mg P per L. Under these conditions, MgO-BC achieved approximately 99.5% phosphate removal. Equilibrium data over an extended initial phosphate concentration range (15-500 mg P per L) were best described by the nonlinear Langmuir isotherm (q max = 11.42 ± 0.11 mg P g-1, K L = 22.43 ± 1.58 L mg-1, R 2 = 0.985), confirming high-affinity, monolayer uptake on a finite number of Mg-rich sites, whereas the nonlinear Freundlich and Temkin models provided inferior fits (R 2 = 0.729 and 0.795, respectively). These model fits, combined with spectroscopic and XRD evidence for Mg-phosphate interactions, are consistent with a mechanism dominated by high-affinity surface reactions rather than weak physisorption. XRD patterns before and after adsorption confirmed that the main reflections of MgO/Mg(OH)2 did not shift after adsorption, indicating that the immobilization of phosphate was mainly due to inner-sphere complexation and poorly crystalline surface precipitation and not to bulk phase transformation. The initial phosphate removal efficiency of MgO-BC was found to be over 80% after five adsorption-desorption cycles, which confirms good regeneration potential. Based on these results, MgO-BC could be identified as an effective and reusable phosphate removal and recovery sorbent from aqueous systems.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Iron–Magnesium Bimetallic Biochar Composites Derived from Conocarpus Waste for Enhanced Phosphate Removal: Insights into the Underlying Adsorption Mechanisms in Aqueous SolutionSustainability · 2026
- MgO-Biochar for Selective Orthophosphate Removal from Swine Wastewater: Optimization and Environmental Assessment.Langmuir : the ACS journal of surfaces and colloids · 2026
- Comparative Phosphate Recovery from Synthetic Solution and Anaerobic Digestion Centrate Using Calcium- and Magnesium-Modified Commercial Biochar: Performance, Adsorption Behavior, and Preliminary Agronomic EvaluationApplied Sciences · 2026
- Adsorption of phosphates on a novel eggshell Ca-modified anaerobic sludge-based biochar: Adsorption performance and mechanismPLoS ONE · 2025
- RSM-optimized Mg/Al-LDH biochar composite for enhanced phosphorus removal: Insights into interlayer structure evolution and adsorption mechanismJournal of Environmental Management · 2026
- Hybrid biochar/layered double oxide for phosphate and humic acid removal from water: dominant role of memory-effect-driven anion intercalation.RSC advances · 2026