Hybrid biochar/layered double oxide for phosphate and humic acid removal from water: dominant role of memory-effect-driven anion intercalation.
Racha Kara, Abdelkader Ouakouak, Lynda Hecini, Dhirar Ben Salem, Noureddine Rouahna, Fouzia Touahra, Nesrine Zenidi, David Houivet,
Research Laboratory in Subterranean and Surface Hydraulics, University of Biskra PO Box 145 Biskra 07000 Algeria racha.kara@univ-biskra.dz. · Scientific and Technical Research Center for Arid Areas (CRSTRA) M.B. 1682 Biskra 07000 Algeria.
Key points
From the paper's conclusion- These findings demonstrate that the biochar/LDO composite is a promising low-cost and reusable adsorbent for the simultaneous removal of organic and inorganic contaminants from wastewater.
Abstract
A biochar/layered double oxide (LDO) composite was successfully developed for the simultaneous removal of phosphate (P) and humic acid (HA) from aqueous solutions. The composite was synthesised by in situ co-precipitation of Mg2+ and Al3+ salts to form a Mg/Al-layered double hydroxide (Mg/Al-LDH) on palm fibre-derived biochar, followed by calcination at 500 °C. X-ray diffraction confirmed the successful formation of crystalline Mg/Al-LDH with a basal spacing (d 003) of 0.755 nm. The specific surface areas of PF-biochar, biochar/LDH, and biochar/LDO were 465.2, 268.3, and 241.2 m2 g-1, respectively. The Langmuir maximum adsorption capacities for P and HA followed the order: biochar/LDO (28.6 and 152.9 mg g-1) > biochar/LDH (15.0 and 112.7 mg g-1) > PF-biochar (7.40 and 74.1 mg g-1). Thermodynamic analysis showed that the adsorption of P (ΔH° = 15.92 kJ mol-1) and HA (ΔH° = 13.56 kJ mol-1) was endothermic and predominantly governed by physical interactions. XRD analysis of biochar/LDO revealed that the basal spacing of the reconstructed LDH increased from 0.741 nm after rehydration in water to 0.882 nm and 1.147 nm following phosphate and HA adsorption, respectively, demonstrating anion intercalation associated with the memory effect. In addition to the memory effect, phosphate adsorption involved electrostatic attraction and surface complexation, whereas humic acid adsorption additionally involved electrostatic attraction, hydrogen bonding, and π-π interactions. The estimated direct operating cost for preparing the biochar/LDO composite was approximately 1.86 (US$ per kg). These findings demonstrate that the biochar/LDO composite is a promising low-cost and reusable adsorbent for the simultaneous removal of organic and inorganic contaminants from wastewater.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Layered Double Hydroxides/Biochar Composites as Sustainable Adsorbents for Phosphorus Removal in Water: Recent Trends and PerspectivesACS ES&T Engineering · 2026
- Efficient phosphate adsorption from real industrial wastewater using a La/Mg-Fe LDH-biochar integrated guar gum-gelatin hydrogel towards sustainable resource reuse.International journal of biological macromolecules · 2026
- Adsorption of phosphates on a novel eggshell Ca-modified anaerobic sludge-based biochar: Adsorption performance and mechanismPLoS ONE · 2025
- Tailored olive pomace biochar anchored with CaAl layered double oxides for phosphate remediation from food industry wastewater: Role of pyrolysis and mechanistic insightsJournal of Water Process Engineering · 2025
- Engineering MgFe-Layered Double Hydroxide/Biochar Composites from Date Palm Residues for Enhanced Removal of Nitrate, Ammonium, and Phosphate from Aqueous SolutionsInorganics · 2026
- Humic acid–Fe–kaolinite composite for robust phosphate removal from complex wastewater matricesScientific Reports · 2026