Tuning the mechanical integrity and corrosion performance of open-cell copper foams: identification of an optimization threshold
Mohamed Ali Hassan, Omayma A. El-Kady, Moataz H. Ata, Ibrahim Najih, Amr Ali
Key points
From the paper's conclusion- Overall, lower-porosity porous copper foam architectures offer superior structural energy absorption, whereas the 25 wt% NaCl configuration achieves an optimal balance between mechanical integrity and corrosion resistance.
Abstract
In this work, Porous copper foam samples were fabricated by a space-holder technique with water-atomized copper powder and sodium chloride (NaCl) particles in weight fractions ranging from 10 to 35 wt%. The powders were mechanically mixed at a 10:1 ball-to-powder ratio and 150 rpm for 2 h. The effects of space-holder content on the physical, mechanical, tribological, and electrochemical performance were systematically investigated. Increasing the NaCl fraction precisely controlled the total porosity, from 39.15% to 57.76%, and reduced the bulk density from 5.452 to 3.785 g/cm³. XRD and SEM analyses confirmed a single-phase FCC copper matrix and a structural transition from isolated pores to a highly interconnected open-cell network. Consequently, Vickers hardness, compressive yield strength, energy absorption capacity decreased from 52.12 to 29.23 HV, 18.25 to 1.65 MPa, and 35.73 to 10.46 MJ/m³, respectively, following a modified Gibson–Ashby model (R 2 = 0.95). Concurrently, the coefficient of friction and specific wear rate increased (reaching a maximum of 0.73 mm³/N·m under 15 N for 35 wt% NaCl) due to strut thinning and localized delamination. Electrochemical evaluation in 3.5 wt% NaCl solution revealed an optimization threshold for sample fabricated with 25 wt% NaCl, which exhibited the lowest corrosion rate of 0.918 mm/y, and the highest polarization resistance (Rp) of 267.28 Ω, due to a stable Cu 2 O passive film. Exceeding this threshold at 30 and 35 wt% NaCl led to structural instability and stagnant electrolyte zones, accelerating corrosion kinetics. Overall, lower-porosity porous copper foam architectures offer superior structural energy absorption, whereas the 25 wt% NaCl configuration achieves an optimal balance between mechanical integrity and corrosion resistance.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Corrosion and corrosion fatigue studies of PBF-EB/M-manufactured porous iron in simulated body fluidnpj Materials Degradation · 2026
- Ambient Pressure Drying Cellulose-Graphite Foam with Ordered Pores: Mechanical Robustness, Thermal Insulation and Self-Extinguishing Performance.ACS applied materials & interfaces · 2026
- CeO2-Modified Ni201 Laser-Clad Coatings: Wear Behavior and Alkaline Corrosion ResponseLubricants · 2026
- Polydopamine‐Assisted Copper Deposition on Cellulose Nanofiber Composites: Effect of Nanofiber Scaffold Structure on Particle Formation and Sintered ConductivityJournal of Applied Polymer Science · 2026
- Engineering Hierarchically Nano‐Structured Cu Foams: Dynamic Hydrogen Bubble Templated Binder‐Free Freestanding Electrodes for Energy ApplicationsSmall · 2025
- Study on the influence of pore structure on the foam concrete towards sound absorption enhancementConstruction and Building Materials · 2025