Effect of printing layer thickness and sintering time on the densification, microstructure and mechanical properties of binder-jetted Ti-6Al-4V alloy
Shudong Huang, Chengkang Qi, Xiaohan Cui, Zhehan Li, Dawei Guan, Yaozhong Zhang, Weibo Jia, Fei Li
Key points
From the paper's conclusion- This study examines how printing layer thickness and sintering time jointly affect the densification, microstructure, and tensile behavior of binder-jetted Ti-6Al-4V under a fixed jetting strategy.
Abstract
This study examines how printing layer thickness and sintering time jointly affect the densification, microstructure, and tensile behavior of binder-jetted Ti-6Al-4V under a fixed jetting strategy. Specimens were printed with layer thicknesses of 40, 80, and 120 μm and sintered at 1300 °C for 1–5 h. Reducing the layer thickness increased green density and refined the initial pore structure, thereby accelerating pore closure during early sintering. The 40 μm specimens reached the best condition after 2 h, with 94.4% relative density, 4.4% porosity, and an ultimate tensile strength approaches the wrought benchmark. Larger layer thicknesses required longer holding times but showed lower maximum densities within the investigated process window. Prolonged holding also promoted grain growth and possible pore coarsening, which limited further improvement. These results indicate that improving the green-body state by reducing layer thickness is more effective than simply extending sintering time, although ductility and residual defect control remain important for further optimization.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Size-Dependent Mechanical Properties of Additively Manufactured Ti-6Al-4V Thin WallsMaterials · 2026
- Optimization of laser powder bed fusion process to enhance mechanical properties of as-built Ti–6Al–4V samplesJournal of Materials Research and Technology · 2025
- Correlations in LPBF-fabricated Ti6Al4V: Influence of laser power and scanning speed on microstructure and mechanical performanceResults in Engineering · 2026
- Microstructure Evolution and Mechanical Properties of Al0.5Cr0.9FeNi2.5V0.2 High-Entropy Alloy Fabricated by Binder Jetting 3D Printing and Vacuum SinteringMaterials · 2026
- Effect of process parameters on surface integrity in laser powder bed fusion of Ti-6Al-4V alloyScientific Reports · 2025
- Influence of speed sintering on the mechanical properties of layer-free multi-layer zirconia.Dental materials journal · 2026