Activating the Anomalous Jahn-Teller Effect in NASICON-Type Mixed Phosphate Cathode via Crystal Field Engineering.
Peiyao Li, Yingde Huang, Dinghao Le, Yujing Chen, Pei Yang, Tian Chen, Kunmei Yang, Qing Wu,
National Key Laboratory of Energy Metal Resources and New Materials, School of Metallurgy and Environment, Central South University, Changsha, Hunan410083, P. R. China. · School of Materials Science and Engineering, Zhengzhou University, Zhengzhou, Henan450001, P. R. China.
Key points
From the paper's conclusion- This work demonstrates that Jahn-Teller distortion can be rationally re-engineered into a kinetic advantage and provides new insights into the design of high-energy-density NASICON-type cathodes for batteries.
Abstract
High-voltage Mn3+/Mn2+ redox reactions in polyanionic cathodes offer the potential to increase energy density while reducing the cost of batteries. However, its practical application is hindered by sluggish reaction kinetics and asymmetric Jahn-Teller distortion. Herein, we report a NASICON-type cathode, Na3.85□0.15Mn1.35Fe1.5V0.15(PO4)2(P2O7) (□ denotes Na vacancy, NFMPP-V), in which vanadium substitution reconfigures the Mn3+-induced Jahn-Teller distortion and couples it with multivalent redox processes, achieving enhanced energy density and reaction kinetics. Remarkably, the Na+ mobility increases with the Jahn-Teller distortion, exhibiting an anomalous behavior opposite to that of conventional Mn-based cathodes, which is associated with an ordered anisotropic distortion of the [MnO6] octahedra. As a result, NFMPP-V delivers a high reversible capacity of 120.2 mAh g-1 and achieves a capacity retention of 82.3% for 500 cycles at 5C. This work demonstrates that Jahn-Teller distortion can be rationally re-engineered into a kinetic advantage and provides new insights into the design of high-energy-density NASICON-type cathodes for batteries.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Interfacial Electronic-Structural Coupling Suppresses Jahn-Teller Instability in NASICON Cathode Casting Long Cycling Life.Advanced materials (Deerfield Beach, Fla.) · 2026
- Reduced Bond Covalency and Anisotropic Lattice Distortion Enable High Fe–Mn Redox Activation in a Mixed-Polyanionic CathodeACS Nano · 2025
- Mitigating P2 - P2' phase transition and lattice oxygen loss toward high-performance Fe/Mn-based Na-ion layered cathodes.Journal of colloid and interface science · 2026
- Re‐Evaluating Jahn–Teller Distortion for Structural Flexibility and Fast Ion Transport in LMFP CathodesAdvanced Functional Materials · 2026
- Jahn–Teller Distortion Triggers Unconventional Molecular O 2 Formation in P2‐Type Na 0.67 MnO 2 CathodesAdvanced Functional Materials · 2026
- Enabling Ultrahigh-Power-Density LiMn0.6Fe0.4PO4 Cathodes via Kinetics Limitation Breakthrough and Jahn-Teller Distortion Mitigation.ACS nano · 2026