Synergistic V-Mg Co-Doping for a High-Manganese LiMn0.9Fe0.1PO4 Cathode with Superior Cycling Stability and Rate Capability.
Cheng Zhang, Yida Wang, Long Ye, Xin Zeng, Yixin He, Juntao Si, Sihan Zeng, Bicai Pan,
State Key Laboratory of Precision and Intelligent Chemistry, Department of Materials Science and Engineering, University of Science and Technology of China, Hefei, Anhui230026, P.R. China. · Hefei National Laboratory for Physical Sciences at the Micro Scale, Key Laboratory of Strongly-Coupled Quantum Matter Physics, Department of Physics, University of Science and Technology of China, Hefei, Anhui230026, P.R. China.
Key points
From the paper's conclusion- High-manganese lithium manganese iron phosphate (LiMn0.9Fe0.1PO4, 9Mn-LMFP) offers a high-voltage platform for high-energy-density Li-ion batteries but suffers from poor electronic conductivity, Mn dissolution, and structural degradation.
Abstract
High-manganese lithium manganese iron phosphate (LiMn0.9Fe0.1PO4, 9Mn-LMFP) offers a high-voltage platform for high-energy-density Li-ion batteries but suffers from poor electronic conductivity, Mn dissolution, and structural degradation. Herein, we report a V-Mg co-doping strategy via one-step ball milling combined with solid-state sintering to address these challenges. V3+ incorporation narrows the band gap from 3.39 to 1.34 eV and promotes a uniform and dense carbon coating on the particle surface. Mg2+ stabilizes the crystal framework, as evidenced by shortened Mn-O bonds and reduced Mn dissolution (from 6.128 to 3.139 ppm). Furthermore, V-Mg co-doping expands the solid-solution region (from 44.1 to 48.1% state of charge) while shrinking the two-phase region, indicating a lowered phase-transformation barrier. Consequently, the 9Mn-LMFP-V-Mg∥Li half-cells exhibit optimal electrochemical performance with a discharge capacity of 157.0 mAh g-1 at 0.1C, 123.7 mAh g-1 at 10C, and 89.7% capacity retention after 400 cycles at 1C, significantly outperforming the undoped counterpart (with a capacity retention of only 58.2%). When paired with the Li4Ti5O12 anode, 9Mn-LMFP-V-Mg delivers 118.6 mAh g-1 at 2C with 82.5% retention after 100 cycles. Kinetic analyses reveal reduced charge transfer resistance, enhanced Li+ diffusivity (approximately one order of magnitude higher), and increased pseudocapacitive contribution, leading to minimized polarization and efficient capacity release under high rates. This work provides a viable strategy for developing high-energy-density, long-life olivine cathodes.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Heterocations Synergistic Doping for Kinetically Enhanced and Structurally Stable LiMn 0.6 Fe 0.4 PO₄ACS Applied Materials & Interfaces · 2026
- Orbital Engineering via D‐p Hybridization by in Doping Enables High‐Performance Lithium Manganese Iron Phosphate CathodesAdvanced Functional Materials · 2026
- Spin-State Engineering of Manganese Boosts the Electrochemical Performance of LiFe0.2Mn0.8PO4 Cathodes.Journal of the American Chemical Society · 2026
- Enhanced electrochemical performance of LiMn0.6Fe0.4PO4/C via Co and Ti dual-doping with gradient structural designJournal of Power Sources · 2026
- Gradient Mg and Uniform Ti Co‐Doping Suppresses Jahn–Teller Effect in LMFP via Optimized Ion‐Transport Kinetics and Interfacial ReactionsAngewandte Chemie International Edition · 2026
- Mitigating Mn‐Driven Interfacial Instability in LiMn 0.5 Fe 0.5 PO₄ Cathodes for Lithium‐Ion Batteries via Surface‐Intensive Ta DopingSmall · 2026