Early-Stage Thermal Safety Evaluation of the NMC811/LLZO/Li Solid-State Battery Chemistry Using Calorimetry and Characterization Methods
Zixuan Wang, Bhuvsmita Bhargava, Nathan Brenner Johnson, Alex Bates, Loraine Torres-Castro, M Florencia Petracci, Michael Grady McKee, W. K. Schubert,
University of Maryland, College Park · Sandia National Laboratories
Key points
From the paper's conclusion- We compare solid-state material sets with a Li metal anode and LLZO separator and either NMC811 or lithium cobalt oxide cathode and find that thermal metrics such as the total heat release and the onset temperatures are broadly similar, reflecting a common exothermic reaction path involving oxygen release from layered oxide cathode active materials and HF release from the PVDF binder and their rea
Abstract
With the emergence of various battery chemistries including lithium metal solid-state batteries, early-stage safety evaluations can provide insights into designs for safe material sets, cells, and packs. Differential scanning calorimetry (DSC) can be performed to determine the heat flow of small (<10 mg) samples. We construct hermetically sealed Li/LLZO/NMC811 anode-cathode-electrolyte (ACE) solid-state samples for DSC tests and measure the onset temperature of exothermic reactions, the rate of heat flow, and the total heat released by 500 °C. Proposed chemical reaction pathways are constructed using a mass-energy balance from DSC and TGA, with additional input from other characterization methods. By adding an isothermal hold at the end of the constant rate heating in DSC tests (500 °C in our protocol), we obtain additional heat flow important for determining the reaction pathways. We find that our NMC811/LLZO/Li ACE samples have a total heat release of ∼15 J/mAh at 500 °C with an onset temperature of around 220 °C. We compare solid-state material sets with a Li metal anode and LLZO separator and either NMC811 or lithium cobalt oxide cathode and find that thermal metrics such as the total heat release and the onset temperatures are broadly similar, reflecting a common exothermic reaction path involving oxygen release from layered oxide cathode active materials and HF release from the PVDF binder and their reaction with reductants including lithium metal and conductive carbon.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Thermal Stability of LiNiₓ Mn y Co z O₂ Cathode MaterialsChemistry of Materials · 2026
- Assessing the Safety of Solid-State Technologies: What Can We Learn from a Coin CellACS Applied Energy Materials · 2026
- Thermal Stability Landscape of Solid-State BatteriesACS Energy Letters · 2026
- Solid-Ejecta Morphology and Elemental Composition During Thermal Runaway of 58 Ah NCM811 Lithium-Ion Cells: Representative Near-Field Thermal-Flow Behavior.Materials (Basel, Switzerland) · 2026
- A multiscale X-ray CT study of degradation and safety behaviour of different Li-ion battery positive electrode morphologies.EES batteries · 2026