A multiscale X-ray CT study of degradation and safety behaviour of different Li-ion battery positive electrode morphologies.
Hamish T Reid, Drasti Patel, Will J Dawson, James B Robinson, Rhodri Jervis, Paul R Shearing
Electrochemical Innovation Lab (EIL), Department of Chemical Engineering, University College London (UCL) London WC1E 7JE UK paul.shearing@eng.ox.ac.uk. · Advanced Propulsion Lab (APL), Marshgate, UCL London E20 2AE UK.
Key points
From the paper's conclusion- Electrochemical testing accelerating rate calorimetry (ARC), and multiscale X-ray computed tomography (CT) are combined to investigate how state-of-safety of lithium-ion pouch cells containing single-crystal or polycrystalline NMC cathode evolves with cycling.
- The single-crystal containing cells gave an approximate 50% improvement in cycle life compared with polycrystalline cells. In the pristine state, ARC showed that the single-crystal cells had a lower self-heating onset temperature but also a lower peak temperature than polycrystalline cells, indicating lower thermal stability but less destructive failure. After cycling, the single-crystal cells showed higher self-heating onset temperature and lower peak temperatures.
- Whole-cell imaging revealed greater gas generation, electrode displacement, and loss of layer contact in the polycrystalline cells, while high-resolution CT identified extensive particle cracking and fragmentation that was largely absent in the single-crystal material, suggesting that ageing-induced particle fracture increases the reactive cathode-electrolyte interfacial area, accelerating exothermic reactions during thermal abuse and reducing thermal stability.
Abstract
While battery thermal failures are rare, improving our understanding of battery state-of-safety is essential to further reduce failure rates and support the energy transition. Although batteries undergo rigorous certification, the evolution of safety characteristics with cell ageing remains poorly understood. Here, electrochemical testing accelerating rate calorimetry (ARC), and multiscale X-ray computed tomography (CT) are combined to investigate how state-of-safety of lithium-ion pouch cells containing single-crystal or polycrystalline NMC cathode evolves with cycling. Comparable pouch cells were assessed before and after cycling to 80% capacity retention. The single-crystal containing cells gave an approximate 50% improvement in cycle life compared with polycrystalline cells. In the pristine state, ARC showed that the single-crystal cells had a lower self-heating onset temperature but also a lower peak temperature than polycrystalline cells, indicating lower thermal stability but less destructive failure. After cycling, the single-crystal cells showed higher self-heating onset temperature and lower peak temperatures. In contrast, the polycrystalline cells showed reduced self-heating onset temperatures and thermal runaway initiation temperatures indicating a loss of thermal stability. Multiscale X-ray CT provided mechanistic insight into these changes by linking safety behaviour to degradation across multiple length scales. Whole-cell imaging revealed greater gas generation, electrode displacement, and loss of layer contact in the polycrystalline cells, while high-resolution CT identified extensive particle cracking and fragmentation that was largely absent in the single-crystal material. These observations suggest that ageing-induced particle fracture increases the reactive cathode-electrolyte interfacial area, accelerating exothermic reactions during thermal abuse and reducing thermal stability. This work demonstrates how multiscale X-ray CT can reveal the mechanisms that influence the changes in of battery state-of-safety with cycling and highlights the potential safety advantages of single-crystal cathode architectures in aged lithium-ion batteries.
Read the paper
Discussion · 1
Science Skim's AI key points, plus readers' public thoughts
- Electrochemical testing accelerating rate calorimetry (ARC), and multiscale X-ray computed tomography (CT) are combined to investigate how state-of-safety of lithium-ion pouch cells containing single-crystal or polycrystalline NMC cathode evolves with cycling.
- The single-crystal containing cells gave an approximate 50% improvement in cycle life compared with polycrystalline cells. In the pristine state, ARC showed that the single-crystal cells had a lower self-heating onset temperature but also a lower peak temperature than polycrystalline cells, indicating lower thermal stability but less destructive failure. After cycling, the single-crystal cells showed higher self-heating onset temperature and lower peak temperatures.
- Whole-cell imaging revealed greater gas generation, electrode displacement, and loss of layer contact in the polycrystalline cells, while high-resolution CT identified extensive particle cracking and fragmentation that was largely absent in the single-crystal material, suggesting that ageing-induced particle fracture increases the reactive cathode-electrolyte interfacial area, accelerating exothermic reactions during thermal abuse and reducing thermal stability.
Readers' thoughts
No reader thoughts yet.
Related papers
- Failure Characteristics of Cylindrical Cells (18650 and 26700) Across Sodium-Ion, Lithium Nickel Manganese Cobalt Oxide (NMC), Lithium Iron Phosphate (LFP) and Lithium Titanate (LTO) ChemistriesBatteries · 2026
- Evolution of safety risks during battery degradation: Mechanisms and implicationsJournal of Energy Chemistry · 2026
- Thermal Stability of LiNiₓ Mn y Co z O₂ Cathode MaterialsChemistry of Materials · 2026
- Thermal Stability and Gas Evolution of Li-Rich Mn-Based Cathodes and Their Links to Cell-Level Thermal Runaway: A ReviewBatteries · 2026
- Post-Synthetic Cerium Modification of Commercial NCM811 for Concurrent Cycling and Safety Upgrading.Advanced science (Weinheim, Baden-Wurttemberg, Germany) · 2026
- Cross-Dataset Assessment of Cathode Thermal Descriptors for Whole-Cell Self-Heating Kinetics in Lithium-Ion Batteries: Onset, Reaction Magnitude, and Limits of TransferabilityBatteries · 2026