Plasma-Polymerized Coatings Retaining Oxidized-Sulfur Functionalities for Liquid-Interface Applications
Nepal C. Roy, Güsta Irem Sakiz, Elahe Naghdi, David Petitjean, Filip Legein, Wim De Malsche, Francois Reniers
Key points
From the paper's conclusion- Overall, these findings identify sulfur leaching and coating removal as distinct failure modes and provide a materials-design strategy for durable plasma-polymer coatings that retain cation-exchange functionalities under liquid flow.
Abstract
Plasma polymerization enables the synthesis of functional coatings; however, poor retention of functional groups during extended liquid exposure can limit their performance at solid−liquid interfaces. Here, a hybrid precursor chemistry was combined with rapid thermal annealing (RTA) to retain oxidized sulfur within a carboxyl-rich plasma-polymer matrix. To this end, sulfur-containing coatings were deposited on silicon in a single step by atmospheric-pressure dielectric barrier discharge plasma polymerization. The precursors were trifluoromethanesulfonic acid (TFMSA), sodium 4-styrenesulfonate with ethylene glycol (NaSS + EG), and a hybrid precursor (HP) comprising H2SO4 and S8 in acrylic acid (AA), while AA alone served as the sulfur-free reference. X-ray photoelectron spectroscopy (XPS), supported by infrared reflection−absorption spectroscopy (IRRAS), distinguished reduced and oxidized sulfur species. Upon liquid exposure, the TFMSA- and NaSS + EG-derived coatings rapidly lost most of their sulfur, consistent with leaching of weakly bound sulfur-containing species. By contrast, the HP-derived coatings retained oxidized sulfur within the AA-derived matrix but were gradually removed from the substrate under continuous flow. A 10 s RTA pulse at a 440 °C set point, however, prevented this failure. The annealed coating preserved its substrate coverage, near-surface sulfur content, and oxidized-sulfur fraction during 168 h of continuous flow in acetate buffer (pH 5.5). Although annealing reduced the overall sulfur content (2.8 → 1.7 at %), it markedly improved coating durability. Overall, these findings identify sulfur leaching and coating removal as distinct failure modes and provide a materials-design strategy for durable plasma-polymer coatings that retain cation-exchange functionalities under liquid flow.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Interfacial engineering of surface-functionalized hydroxyapatite@Ag nanohybrids for sensitive SERS detection.Spectrochimica acta. Part A, Molecular and biomolecular spectroscopy · 2026
- Microstructural Evolution and Failure Mechanisms of Plasma-Sprayed Pure Si and Si–15 mol% HfO2 Bond Coatings in Dry-Oxygen and Water-Vapor Environments at 1623 KCoatings · 2026
- Microstructure engineering of sol-gel SiO2 coatings with biomass derived carbon dots for enhanced corrosion protection of stainless steel.RSC advances · 2026
- Sulfur(VI) Fluoride Exchange Chemistry in Polymer Functionalization: Post-Polymerization Modification, Interface Engineering, and Biopolymer Conjugation.Molecules (Basel, Switzerland) · 2026
- Corrosion and Biofouling Protection via a Spatial-Temporal Strategy Enabled by Barrier and Liquid-Like Interfaces in Ultrathin PECVD Coatings.Small (Weinheim an der Bergstrasse, Germany) · 2026
- Cyclic Olefin Copolymer with a Noble Metal Nanostructures as an Antibacterial MaterialInternational Journal of Molecular Sciences · 2026