Time-Resolved Structural Insight into Zinc Metal Plating in Aqueous Batteries.
Lacey Roberts, Claire Ely, Elizabeth Allan-Cole, Julian Mars, Thomas Chaney, Denis Keane, Saul Lapidus, Erik Sarnello,
Department of Chemical and Biological Engineering, University of Colorado Boulder, Boulder, Colorado 80303, United States. · Materials Science and Engineering, University of Colorado, Boulder, Colorado 80303, United States.
Key points
From the paper's conclusion- Here, we use operando X-ray diffraction to track zinc plating and stripping under varying current densities and capacities, uncovering key structural changes that govern reversibility.
Abstract
Zinc metal anodes are promising for next-generation aqueous batteries due to their low electrochemical potential, high volumetric capacity, and global abundance. However, their application is hindered by irreversibility caused by parasitic reactions on the anode, including hydrogen evolution, dendrite formation, and zinc hydroxide sulfate (ZHS) buildup. The structural origins of electrochemical irreversibility in aqueous zinc cells are related to these parasitic side reactions, plating/stripping efficiency, and the crystallographic evolution of zinc anodes during cycling. Here, we use operando X-ray diffraction to track zinc plating and stripping under varying current densities and capacities, uncovering key structural changes that govern reversibility. Zinc plates with a preferred (002) orientation during the first cycle; however, subsequent cycling disrupts this texture, especially at high capacities, shifting the orientation toward Zn(100) or producing random orientations. We show that ZHS formation is governed primarily by the total time spent at low potentials rather than current density or cycle number, implicating calendar aging as a dominant degradation pathway. Dead zinc and ZHS formation both correlate with reduced Coulombic efficiency, but dead zinc appears to be the dominant factor in early cycle reversibility loss. These findings provide structural insight into degradation mechanisms and highlight the importance of engineering interfaces and electrolytes to control crystallographic orientation and parasitic phase formation.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- From Plating‐Centric to Full‐Cycle Design: A Perspective on the Critical Role of Zinc Anode StrippingAdvanced Materials · 2026
- Zinc utilization rate in aqueous batteries: Regulation of interfacial thermodynamics and kineticsNational Science Open · 2025
- Challenges of Zn anode under stringent conditions and improvement strategiesNexus · 2025
- Facet-Dependent Plating/Stripping Behavior and Crystallographic Evolution during Cycling on Zn Metal AnodesACS Energy Letters · 2026
- Interface-Induced Crystallographic Orientation of Zinc Deposition Enabled by a Zwitterionic Dynamic Buffering Interface for Ultralong-Life Aqueous Zinc Batteries.Nano letters · 2026
- Electric Double Layer‐Driven Surface Reconstruction Enables Cooperative Zn(002)/(101) Growth for High‐Utilization Zinc AnodesAdvanced Energy Materials · 2026