From the paper's conclusion
  • This synergistic chemisorbed-mobile-ion buffering network thickens the electric double layer, inhibits water-splitting parasitic reactions, and induces (101)-oriented deposition.

Abstract

The development of aqueous zinc batteries is critically constrained by the electrode-electrolyte interfacial instability at the Zn anode. Herein, a zwitterionic dynamic buffering interface (ZDBI) is constructed by using trace glufosinate ammonium (GA). The dissociated GA- anchors onto the Zn(101) surface via its phosphinate and carboxylate groups with its protonated amino group (-NH3+) extending into the electrolyte to dynamically respond to interfacial electric fields. Meanwhile, free NH4+ cations can form an electrostatic shielding layer under an electric field. This synergistic chemisorbed-mobile-ion buffering network thickens the electric double layer, inhibits water-splitting parasitic reactions, and induces (101)-oriented deposition. Consequently, Zn||Zn symmetric cells sustain stable cycling for over 7800 h with a cumulative capacity of 3.9 Ah cm-2, while Zn||Cu half-cells achieve an average Coulombic efficiency of 99.3%, and Zn||V2O5 full cells retain 88% capacity after 1000 cycles at 5 A g-1. This work offers an efficient strategy for addressing electrode-electrolyte interfacial issues.